Abstract
To extend the oxidation protective temperature range of coating for carbon/carbon (C/C) composites, a SiC/ZrB 2-SiC/SiC multilayer coating was prepared by a three-step method of pack cementation, slurry and chemical vapor deposition. The prepared coating is composed of three layers with about 150μm in thickness. It can protect C/C composites from oxidation for more than 300h at 1173K which is attributed to the oxidation ability of ZrB 2. The coating can also effectively protect C/C composites from oxidation at 1773K for 217h which is due to the SiO 2-ZrSiO 4 compound glass during oxidation test.
Original language | English |
---|---|
Pages (from-to) | 148-153 |
Number of pages | 6 |
Journal | Corrosion Science |
Volume | 57 |
DOIs | |
State | Published - Apr 2012 |
Keywords
- A. Ceramic
- B. Thermal cycling
- B. Weight loss
- C. Oxidation