金属表面HVOF碳化钨金属陶瓷涂层的疲劳寿命研究进展

Translated title of the contribution: Research Progress on Fatigue Life of HVOF Tungsten Carbide Cermet Coating

Shouchang Ji, Jinglong Li, Dan Chen, Zhengxian Li, Haiyu Yang

Research output: Contribution to journalReview articlepeer-review

1 Scopus citations

Abstract

High velocity oxygen fuel (HVOF) sprayed WC cermet coating possesses high hardness, high bonding strength and nearly full-density, which are the candidates of EHC (electrolytic hard chromium). In the present paper, the research status quo of the influence of HVOF sprayed WC coating on the fatigue life of the substrate was summarized and the reasons of crack initiation and fatigue life decrease were also analyzed. The factors affecting the fatigue life are as follows: the difference between the coating and the substrate in properties, the defects introduced by grit blasting, residual stress and coating preparation. The improvement measures include coating gradient design, change of the pre-treatment such as shot peening replacing grit blasting, obtaining or increasing the coating compressive stress, reducing the decomposition of carbide, reasonable process parameters (such as high speed), proper coating thickness, applying WC powder with high content of binder, appropriate post-treatment of the coating.

Translated title of the contributionResearch Progress on Fatigue Life of HVOF Tungsten Carbide Cermet Coating
Original languageChinese (Traditional)
Pages (from-to)4539-4552
Number of pages14
JournalXiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering
Volume50
Issue number12
StatePublished - Dec 2021

Fingerprint

Dive into the research topics of 'Research Progress on Fatigue Life of HVOF Tungsten Carbide Cermet Coating'. Together they form a unique fingerprint.

Cite this