N2 - In this study, a metastable β Ti–7Mo–3Al–3Cr–3Nb alloy with αs+β microstructure shows both TRIP and TWIP effects. Although the alloy has a low yield strength of 433 MPa, it shows a high work hardening rate of approximately 8.3 GPa. Besides, it has a total elongation of nearly 20 %. The deformation mechanism was systematically investigated by combining EBSD and TEM analysis on specimens with tensile strains of 1.7 %, 3.5 %, 8.3 %, until failure. The primary deformation mechanisms during tensile deformation are stress-induced α′′ martensitic transformation and dislocation slip. At strain initiation stage stress-induced lath martensite forms, accompanied by its growth, widening, and merging. At medium strain levels, martensitic domains form, accompanied by the appearance of a small number of martensitic twins. At high strain levels, a significant increase in martensitic twins is observed. The high work hardening rate is attributed to the continuous cutting of the β phase by martensitic variants that growing in different directions under low strain levels, which leads to a dynamic Hall-Petch effect. In the later stages of deformation, various types of martensitic twins form within the martensite domain until the matrix β phase is exhausted, playing a crucial role in achieving significant uniform elongation.
AB - In this study, a metastable β Ti–7Mo–3Al–3Cr–3Nb alloy with αs+β microstructure shows both TRIP and TWIP effects. Although the alloy has a low yield strength of 433 MPa, it shows a high work hardening rate of approximately 8.3 GPa. Besides, it has a total elongation of nearly 20 %. The deformation mechanism was systematically investigated by combining EBSD and TEM analysis on specimens with tensile strains of 1.7 %, 3.5 %, 8.3 %, until failure. The primary deformation mechanisms during tensile deformation are stress-induced α′′ martensitic transformation and dislocation slip. At strain initiation stage stress-induced lath martensite forms, accompanied by its growth, widening, and merging. At medium strain levels, martensitic domains form, accompanied by the appearance of a small number of martensitic twins. At high strain levels, a significant increase in martensitic twins is observed. The high work hardening rate is attributed to the continuous cutting of the β phase by martensitic variants that growing in different directions under low strain levels, which leads to a dynamic Hall-Petch effect. In the later stages of deformation, various types of martensitic twins form within the martensite domain until the matrix β phase is exhausted, playing a crucial role in achieving significant uniform elongation.
KW - Deformation mechanism
KW - Metastable β titanium alloy
KW - Stress induced α′′ martensite and martensite twins
KW - α+β structure
UR - https://www.scopus.com/pages/publications/105026133735
U2 - 10.1016/j.jmrt.2025.05.216
DO - 10.1016/j.jmrt.2025.05.216
M3 - 文章
AN - SCOPUS:105026133735
SN - 2238-7854
VL - 36
SP - 10169
EP - 10182
JO - Journal of Materials Research and Technology
JF - Journal of Materials Research and Technology
ER -