Wear resistance enhancement in titanium matrix composites via in‐situ synthesized TiBw by laser melting deposition

  • Chunlun Chen
  • , Liu Deliang
  • , Xiaoli Fan
  • , Kang Guo
  • , Qitao Geng
  • , Luyun Li
  • , Jiang Ju
  • , Jun Wang
  • , Raul Navio Gilaberte
  • , Yan Liu
  • , Zhenlin Zhang
  • , Baode Sun
  • , Hui Chen
  • Southwest Jiaotong University
  • Shanghai Jiao Tong University
  • Alia Energy Consulting S.L.
  • High-end Equipment Advanced Materials and Manufacturing Technology Laboratory

科研成果: 期刊稿件 › 文章 › 同行评审

摘要

With the widespread application of titanium alloys in aerospace equipment, it is imperative to improve wear resistance. In this study, TiBw/TC11 titanium matrix composites were in-situ fabricated by laser melting deposition, and their microstructure and mechanical properties were systematically investigated. The effect of BN addition on the friction and wear behavior of titanium alloys was elucidated by multi-scale characterization. The results show that with increasing BN content, the amount of acicular and short rod-like TiB reinforcements generated by in-situ reaction increases and becomes dispersedly distributed at grain boundaries and α/β lamellar interfaces. The growth of original coarse columnar grains is effectively suppressed by the pinning effect of TiB. Meanwhile, the microhardness of the composites increases progressively from 370.22 HV for TC11–425.65 HV. The composites exhibit distinctly different wear behaviors at room temperature and elevated temperatures. At room temperature, the improvement in wear resistance by BN addition is relatively modest. In contrast, under high‑temperature conditions, the wear mass loss decreases continuously with increasing BN addition. Notably, the 2.0 wt% BN + TC11 sample exhibits a high‑temperature wear mass loss of only 35.1 mg, which is 35.4% lower than that of the TC11 matrix. This marked difference is mainly attributed to the formation of an oxide film on the worn surface of BN‑reinforced samples at elevated temperatures, where the high temperature further promotes the in‑situ formation of Ti₂N hard phase. These findings provide valuable theoretical data and practical references for the further application of titanium matrix composites in aerospace equipment.