  • Xi'an Technological University
  • Northwestern Polytechnical University Xian

科研成果: 期刊稿件文章同行评审

7 引用 (Scopus)

摘要

A spiral fluidity test model of superalloys with 10 mm in height and 3 mm in thickness was designed to evaluate the fluidity of two distinct Ni-based superalloys IN718 and IN939. The factors influencing fluidity are ascertained through comparative analysis utilizing methodologies such as JMatPro, differential scanning calorimetry and high-temperature confocal laser scanning microscopy. The results show that under identical testing conditions, the fluidity of the IN939 superalloy surpasses that of the IN718 superalloy. When subjected to the same temperature, the melt viscosity and surface tension of IN939 superalloy are considerably reduced relative to those of IN718 superalloy, which is beneficial to improving the melt fluidity. Furthermore, the liquidus temperature and solidification range for the IN939 superalloy are both smaller compared with those of the IN718 superalloy. This condition proves advantageous in delaying dendrite coherency, thereby improving fluidity.

源语言英语
页(从-至)2881-2888
页数8
期刊Transactions of Nonferrous Metals Society of China (English Edition)
34
9
DOI
出版状态已出版 - 9月 2024

指纹

探究 'Versatile fluidity test model for cast superalloys and comparison between IN718 and IN939' 的科研主题。它们共同构成独一无二的指纹。

引用此