TY - JOUR
T1 - Transient liquid phase bonding of Ni3Al based superalloy using Mn–Ni–Cr filler
AU - Yuan, Lin
AU - Ren, Jin
AU - Xiong, Jiangtao
AU - Zhao, Wei
AU - Shi, Junmiao
AU - Li, Jinglong
N1 - Publisher Copyright:
© 2021 The Author(s)
PY - 2021/3/1
Y1 - 2021/3/1
N2 - A new 70Mn–25Ni–5Cr (wt. %) filler with no traditional melting-point depressants (MPDs) of Si/B was used for transient liquid phase (TLP) bonding a directionally solidified (DS) superalloy based on Ni3Al intermetallic compound (IMC) at 1150 °C, a pressure of 2 MPa for 10–120 min. Experimental results show that the joint can be divided into 3 zones, isothermally solidified zone (ISZ), athermally solidified zone (ASZ) and diffusion-affected zone (DAZ), which was similar to microstructure of typical TLP joint bonded by Ni based filler. The joint microstructures were mainly composed of γ-Ni, γ′-Ni3(Al, Ta), MC and M23C6 carbides. Besides, in the ISZ, due to the enrichment of Al, which diffused from the base metal (BM), strip-shaped Ni(Mn, Al) phases formed in such region. The ASZ included γ-Ni and compounds of “equiaxed Ni(Mn, Al) + acicular Ni3Ta” owing to the composition segregation during the later stage of solidification. Moreover, as the bonding time increased, the volume fraction of Ni(Mn, Al) and MC carbides decreased owing to homogenization of alloying elements. After bonding for 120 min, sufficient isothermal solidification (IS) of filler can also decrease segregation of Mn/Al in front of the S/L interface and the Ni(Mn, Al)+Ni3Ta compounds were eliminated almost. Thus, the highest tensile strength was 816.9 MPa of the TLP joint of 120 min, which has been equivalent to that of BM (812 MPa). However, due to the existence of a few residual large MC carbides in the joint, which can induce the stress concentration and decreased the ductility of the joints, the highest joint elongation of 4.4% was only about 40% of the BM.
AB - A new 70Mn–25Ni–5Cr (wt. %) filler with no traditional melting-point depressants (MPDs) of Si/B was used for transient liquid phase (TLP) bonding a directionally solidified (DS) superalloy based on Ni3Al intermetallic compound (IMC) at 1150 °C, a pressure of 2 MPa for 10–120 min. Experimental results show that the joint can be divided into 3 zones, isothermally solidified zone (ISZ), athermally solidified zone (ASZ) and diffusion-affected zone (DAZ), which was similar to microstructure of typical TLP joint bonded by Ni based filler. The joint microstructures were mainly composed of γ-Ni, γ′-Ni3(Al, Ta), MC and M23C6 carbides. Besides, in the ISZ, due to the enrichment of Al, which diffused from the base metal (BM), strip-shaped Ni(Mn, Al) phases formed in such region. The ASZ included γ-Ni and compounds of “equiaxed Ni(Mn, Al) + acicular Ni3Ta” owing to the composition segregation during the later stage of solidification. Moreover, as the bonding time increased, the volume fraction of Ni(Mn, Al) and MC carbides decreased owing to homogenization of alloying elements. After bonding for 120 min, sufficient isothermal solidification (IS) of filler can also decrease segregation of Mn/Al in front of the S/L interface and the Ni(Mn, Al)+Ni3Ta compounds were eliminated almost. Thus, the highest tensile strength was 816.9 MPa of the TLP joint of 120 min, which has been equivalent to that of BM (812 MPa). However, due to the existence of a few residual large MC carbides in the joint, which can induce the stress concentration and decreased the ductility of the joints, the highest joint elongation of 4.4% was only about 40% of the BM.
KW - Mechanical properties
KW - Microstructure
KW - NiAl based Superalloy
KW - TLP bonding
UR - https://www.scopus.com/pages/publications/85119205111
U2 - 10.1016/j.jmrt.2021.02.018
DO - 10.1016/j.jmrt.2021.02.018
M3 - 文章
AN - SCOPUS:85119205111
SN - 2238-7854
VL - 11
SP - 1583
EP - 1593
JO - Journal of Materials Research and Technology
JF - Journal of Materials Research and Technology
ER -