The thickness dependence of microstructure, mechanical and wear properties of TiO2coatings formed on Ti-6Al-4V substrate through pulsed anodization

  • Yating Liu
  • , Tao Wang
  • , Hui Liu
  • , Qun Huang
  • , Chao Xu
  • , Weihao Wang
  • , Lu Yan
  • , Binbin Liu
  • Northwestern Polytechnical University Xian
  • Ltd.
  • University of Science and Technology Beijing
  • Beijing Institute of Astronautical Systems Engineering

科研成果: 期刊稿件 › 文章 › 同行评审

摘要

TiO2 coatings with nominal thickness of 2, 4 and 6 µm were fabricated on Ti-6Al-4V substrate via pulsed anodization. The coatings consistently exhibited a mixture of anatase and rutile TiO2 phases, regardless of thickness. All the coatings exhibited volcanic-like porous topography, with the average pore size decreasing as the coating thickness increased. No obvious delamination occurred at the interface between the substrate and TiO2 coating, implying good interfacial bonding. The micro-Vickers hardness (Hv0.5) of TiO2 coating increased with thickness, reaching a value of 570.87 for 6-micron coating. The adhesive strength of 4-micron TiO2 coating was 42.0 MPa, apparently lower than those of 2-micron and 6-micron TiO2 coatings of 53.1 and 51.8 MPa, respectively. The coefficient of friction also showed strong dependence on the coating thickness. A distinctive wear feature was observed in the 4-micron TiO2 coating, where additional shallow worn tracks appeared on both sides of the primary wear track, leading to a larger wear volume of 6.45 × 107µm3compared to the other two coatings. These findings provide valuable insights for the design of TiO2 coatings via pulsed anodization, particularly for fastener applications.

源语言英语
期刊论文编号140902
期刊Thin Solid Films
卷838
DOI
出版状态已出版 - 15 3月 2026