The preparation and mechanical properties of carbon-carbon/lithium-aluminum-silicate composite joints

  • Northwestern Polytechnical University Xian

科研成果: 期刊稿件文章同行评审

27 引用 (Scopus)

摘要

Silica carbide modified carbon cloth laminated C-C composites have been successfully joined to lithium- aluminum-silicate (LAS) glass-ceramics using magnesium-aluminum-silicate (MAS) glass-ceramics as interlayer by vacuum hot-press technique. The microstructure, mechanical properties and fracture mechanism of C-C/LAS composite joints were investigated. SiC coating modified the wettability between C-C composites and LAS glass-ceramics. Three continuous and homogenous interfaces (i.e. C-C/SiC, SiC/MAS and MAS/LAS) were formed by element inter diffusions and chemical reactions, which lead to a smooth transition fromC-C composites to LAS glass-ceramics. The C-C/LAS joints have superior flexural property with a quasi-ductile behavior. The average flexural strength of C-C/LAS joints can be up to 140.26 MPa and 160.02 MPa at 25 ° C and 800 ° C, respectively. The average shear strength of C-C/LAS joints achieves 21.01 MPa and the joints are apt to fracture along the SiC/MAS interface. The high retention of mechanical properties at 800 ° C makes the joints to be potentially used in a broad temperature range as structural components.

源语言英语
页(从-至)346-353
页数8
期刊Materials and Design
44
DOI
出版状态已出版 - 2013

指纹

探究 'The preparation and mechanical properties of carbon-carbon/lithium-aluminum-silicate composite joints' 的科研主题。它们共同构成独一无二的指纹。

引用此