TY - JOUR
T1 - The effect of hBN additive on the microstructure and mechanical properties of sialon ceramics
AU - Li, Daiheng
AU - Zhang, Ping
AU - Wei, Ziyao
AU - Xu, Xiaoyu
AU - Xu, Jie
AU - Gao, Feng
N1 - Publisher Copyright:
© 2025 Elsevier Ltd
PY - 2026/1
Y1 - 2026/1
N2 - While ceramic cutting tools currently offer significant advantages, the complex microstructure and inherent grain growth mechanism of ceramic materials severely limits their application. In this work, Ym/3Si12-(m+n)Alm+nOnN16-n (Sialon, m = 1.2, n = 1.0) ceramics with hexagonal boron nitride (hBN) additive were fabricated by spark plasma sintering. The effect of the particle size and the content of hBN on the microstructure, the hardness, and the fracture toughness of Sialon ceramics have been investigated. The results indicate that the properties of hBN/Sialon materials initially improve followed by a decline as the hBN particle size increases, with the optimal performance observed at a medium particle size (4–6 μm). hBN particulates within Sialon grains, intergranular Y-rich glassy phases and fibrous carbon-rich Sialon-C whiskers were observed. As the hBN doping content increased, both the hardness and fracture toughness of the material decreased, which is attributed to weak interfacial cracking, crack coalescence, and stress-concentration-induced whisker failure by the complex microstructure. The best-performing sample was doped with 2 wt% of 4–6 μm hBN, achieving a hardness of 25.1 GPa and a fracture toughness of 5.0 MPa·m1/2.
AB - While ceramic cutting tools currently offer significant advantages, the complex microstructure and inherent grain growth mechanism of ceramic materials severely limits their application. In this work, Ym/3Si12-(m+n)Alm+nOnN16-n (Sialon, m = 1.2, n = 1.0) ceramics with hexagonal boron nitride (hBN) additive were fabricated by spark plasma sintering. The effect of the particle size and the content of hBN on the microstructure, the hardness, and the fracture toughness of Sialon ceramics have been investigated. The results indicate that the properties of hBN/Sialon materials initially improve followed by a decline as the hBN particle size increases, with the optimal performance observed at a medium particle size (4–6 μm). hBN particulates within Sialon grains, intergranular Y-rich glassy phases and fibrous carbon-rich Sialon-C whiskers were observed. As the hBN doping content increased, both the hardness and fracture toughness of the material decreased, which is attributed to weak interfacial cracking, crack coalescence, and stress-concentration-induced whisker failure by the complex microstructure. The best-performing sample was doped with 2 wt% of 4–6 μm hBN, achieving a hardness of 25.1 GPa and a fracture toughness of 5.0 MPa·m1/2.
KW - BN additive
KW - Grain morphology
KW - Mechanical properties
KW - Microstructure
KW - Sialon ceramics
UR - https://www.scopus.com/pages/publications/105016096452
U2 - 10.1016/j.ijrmhm.2025.107450
DO - 10.1016/j.ijrmhm.2025.107450
M3 - 文章
AN - SCOPUS:105016096452
SN - 0263-4368
VL - 134
JO - International Journal of Refractory Metals and Hard Materials
JF - International Journal of Refractory Metals and Hard Materials
M1 - 107450