TY - JOUR
T1 - Surface morphology evolution during pulsed selective laser melting
T2 - Numerical and experimental investigations
AU - Zheng, Min
AU - Wei, Lei
AU - Chen, Jing
AU - Zhang, Q.
AU - Li, Jiaqiang
AU - Sui, S.
AU - Wang, Geng
AU - Huang, Weidong
N1 - Publisher Copyright:
© 2019 Elsevier B.V.
PY - 2019/12/1
Y1 - 2019/12/1
N2 - A novel physical model for the selective laser melting (SLM) was proposed, providing insights into the surface morphology evolution in the pulsed SLM process. Both Marangoni effect and recoil pressure, which were the prevailing driving forces for the melt flow, were incorporated in the model. It was found that the melt track was characterized by regular fish scale patterns in pulsed remelting process, due to the periodic variation of the molten pool, while the melt track exhibited with a smooth surface under a continuous laser mode. The effect of the exposure time on the surface morphology was also investigated during pulsed SLM process. It was shown that the longer exposure time could produce greater recoil pressure and sufficient molten liquid, leading to a more congested fish scale patterns. The surface defects such as distortions and breakups were strongly associated with the distribution characteristics of the powders. The partially melted particles which attached to the melt flow were the main reasons to the formation of distortions. And the formation the breakups could be attributed to the local lacking of the powders. The simulated results were in good agreement with the experimental results.
AB - A novel physical model for the selective laser melting (SLM) was proposed, providing insights into the surface morphology evolution in the pulsed SLM process. Both Marangoni effect and recoil pressure, which were the prevailing driving forces for the melt flow, were incorporated in the model. It was found that the melt track was characterized by regular fish scale patterns in pulsed remelting process, due to the periodic variation of the molten pool, while the melt track exhibited with a smooth surface under a continuous laser mode. The effect of the exposure time on the surface morphology was also investigated during pulsed SLM process. It was shown that the longer exposure time could produce greater recoil pressure and sufficient molten liquid, leading to a more congested fish scale patterns. The surface defects such as distortions and breakups were strongly associated with the distribution characteristics of the powders. The partially melted particles which attached to the melt flow were the main reasons to the formation of distortions. And the formation the breakups could be attributed to the local lacking of the powders. The simulated results were in good agreement with the experimental results.
KW - Exposure time
KW - Molten pool evolution
KW - Pulsed selective laser melting
KW - Surface defects
KW - Surface morphology
UR - https://www.scopus.com/pages/publications/85070887804
U2 - 10.1016/j.apsusc.2019.143649
DO - 10.1016/j.apsusc.2019.143649
M3 - 文章
AN - SCOPUS:85070887804
SN - 0169-4332
VL - 496
JO - Applied Surface Science
JF - Applied Surface Science
M1 - 143649
ER -