跳到主要导航 跳到搜索 跳到主要内容

Suppression of peritectic reaction in the undercooled peritectic Fe-Ni melts

  • Y. Z. Chen
  • , F. Liu
  • , G. C. Yang
  • , N. Liu
  • , C. L. Yang
  • , Y. H. Zhou
  • Northwestern Polytechnical University Xian

科研成果: 期刊稿件文章同行评审

32 引用 (Scopus)

摘要

Peritectic Fe-Ni alloys were undercooled using glass fluxing. When subjected to an undercooling (ΔT) beyond a critical value (ΔT* ≈ 130 K), the peritectic reaction, L + δ → γ, normally occurring after primary recalescence, was found to be suppressed. This can be ascribed to a longer incubation time for the occurrence of the peritectic reaction than the time required for solidification of δ phase during post-recalescence, for ΔT > ΔT*.

源语言英语
页(从-至)779-782
页数4
期刊Scripta Materialia
57
8
DOI
出版状态已出版 - 10月 2007