Strengthening/toughening of laminated SiCw/SiC ceramic composites by heat treatment

  • Northwestern Polytechnical University Xian
  • Jilin Institute of Chemical Technology

科研成果: 期刊稿件文章同行评审

16 引用 (Scopus)

摘要

Abstract Laminated SiCw/SiC ceramic composites were prepared by chemical vapor infiltration (CVI) and tape casting, and the effect of heat treatment on mechanical properties of the composites was investigated. By heat-treatment of the whiskers at 1700°C, tensile strength, flexural strength and fracture toughness of the composites were increased obviously. The treatment decreased surface roughness and surface oxygen content of the whiskers, the former increased the strength and the latter increased the toughness. More crack deflection, crack bridging and whisker pull-out were observed on the fracture surface. High-temperature flexural strength of laminated SiCw/SiC ceramic composites decreased slowly above 1500°C in vacuum atmosphere due to the failure interface of whisker/matrix.

源语言英语
文章编号10494
页(从-至)10024-10029
页数6
期刊Ceramics International
41
8
DOI
出版状态已出版 - 1 9月 2015

学术指纹

探究 'Strengthening/toughening of laminated SiCw/SiC ceramic composites by heat treatment' 的科研主题。它们共同构成独一无二的学术指纹。

引用此