TY - JOUR
T1 - Significant enhancement on the mechanical and tribological performances of paper-based friction materials by designing silicone@SiO2 core-shell structure
AU - Ma, Shanshan
AU - Tian, Haochen
AU - Fei, Jie
AU - Li, Hejun
N1 - Publisher Copyright:
© 2022 Wiley Periodicals LLC.
PY - 2022/10/5
Y1 - 2022/10/5
N2 - Under the heavy-loading harsh condition, achieving prominent mechanical and tribological performances of paper-based friction materials are an extreme demand for meeting their application in the braking of vehicles. In this study, modifying carbon fiber with epoxy groups and designing silicone@SiO2 core-shell structure as efficient and feasible strategies, were employed to boost the mechanical and tribological properties of friction materials. The above core-shell hybrid, acted as an effective interfacial linker, contributed to forming strong mechanical interlocks and increasing chemical cross-linking density at the interphase. The tensile and interlaminar shear strength of silicone@SiO2-modified sample were improved by 28.6% and 12.9%, respectively. Meanwhile, the toughness of silicone@SiO2-modified sample showed a 102.82% increase. Moreover, compared with pristine sample, the dynamic friction coefficient of silicone@SiO2-modified sample increased from 0.1020 to 0.1202, while the wear rate decreased from 0.617 × 10−8 cm3 J−1 to 0.432 × 10−8 cm3 J−1.
AB - Under the heavy-loading harsh condition, achieving prominent mechanical and tribological performances of paper-based friction materials are an extreme demand for meeting their application in the braking of vehicles. In this study, modifying carbon fiber with epoxy groups and designing silicone@SiO2 core-shell structure as efficient and feasible strategies, were employed to boost the mechanical and tribological properties of friction materials. The above core-shell hybrid, acted as an effective interfacial linker, contributed to forming strong mechanical interlocks and increasing chemical cross-linking density at the interphase. The tensile and interlaminar shear strength of silicone@SiO2-modified sample were improved by 28.6% and 12.9%, respectively. Meanwhile, the toughness of silicone@SiO2-modified sample showed a 102.82% increase. Moreover, compared with pristine sample, the dynamic friction coefficient of silicone@SiO2-modified sample increased from 0.1020 to 0.1202, while the wear rate decreased from 0.617 × 10−8 cm3 J−1 to 0.432 × 10−8 cm3 J−1.
KW - friction
KW - mechanical properties
KW - resins
KW - surfaces and interfaces
KW - wear and lubrication
UR - https://www.scopus.com/pages/publications/85135124858
U2 - 10.1002/app.52883
DO - 10.1002/app.52883
M3 - 文章
AN - SCOPUS:85135124858
SN - 0021-8995
VL - 139
JO - Journal of Applied Polymer Science
JF - Journal of Applied Polymer Science
IS - 37
M1 - e52883
ER -