Rafting is an important phenomenon of the microstructure evolution in nickel-based single crystal superalloys at elevated temperature. Understanding the rafting mechanism and its effect on the microstructure evolution is of great importance in determining the structural stability and applications of the single crystal superalloys. Phase-field method, which is an excellent tool to analyze the microstructure evolution at mesoscale, has been gradually used to investigate the rafting behavior. In this work, we review the crystal plasticity theory and phase-field method and discuss the application of the crystal plasticity theory and phase-field method in the analysis of the creep deformation and microstructure evolution of the single crystal superalloys.

源语言英语
文章编号1095
页(从-至)1-24
页数24
期刊Crystals
10
12
DOI
出版状态已出版 - 12月 2020

指纹

探究 'Review of γ’ rafting behavior in nickel-based superalloys: Crystal plasticity and phase-field simulation' 的科研主题。它们共同构成独一无二的指纹。

引用此