TY - JOUR
T1 - Response mechanism study of alternate ZrC-10vol.% SiC/ZrC-70vol.% SiC coatings with various sublayer thicknesses for cyclic and long-term thermal exposure
AU - Feng, Guanghui
AU - Yao, Xiyuan
AU - Yu, Yulan
AU - Li, Hejun
N1 - Publisher Copyright:
© 2022
PY - 2023/3/20
Y1 - 2023/3/20
N2 - To explore the influence of sublayer numbers on the structure evolution and thermal stress level, an alternate coating consisting of ZrC-10 vol.% SiC and ZrC-70 vol.% SiC sublayers was designed in this work. With a basically consistent general thickness, three coatings constituted by 2, 4 and 6 sublayers were prepared by plasma spraying, which then were assessed using an oxyacetylene torch under cyclic and long-term exposure. The coating with 6 sublayers was supposed to be the one with the best ablation property, finite element analysis also evidenced its least thermal stress among all these samples. After being ablated for 240 s, the linear and mass ablation rates of the coating with 6 sublayers decreased by 51.27% and 14.41% as compared to that with 4 sublayers. Post-test analysis proved the existence of Si-based products, which help the outmost surface to develop a dense profile. Additionally, the yielded alternate dense/porous scale had a preferable toughness, allowing it to maintain a good integrity.
AB - To explore the influence of sublayer numbers on the structure evolution and thermal stress level, an alternate coating consisting of ZrC-10 vol.% SiC and ZrC-70 vol.% SiC sublayers was designed in this work. With a basically consistent general thickness, three coatings constituted by 2, 4 and 6 sublayers were prepared by plasma spraying, which then were assessed using an oxyacetylene torch under cyclic and long-term exposure. The coating with 6 sublayers was supposed to be the one with the best ablation property, finite element analysis also evidenced its least thermal stress among all these samples. After being ablated for 240 s, the linear and mass ablation rates of the coating with 6 sublayers decreased by 51.27% and 14.41% as compared to that with 4 sublayers. Post-test analysis proved the existence of Si-based products, which help the outmost surface to develop a dense profile. Additionally, the yielded alternate dense/porous scale had a preferable toughness, allowing it to maintain a good integrity.
KW - Alternate coating
KW - Carbon/carbon composites
KW - High-temperature test
KW - Plasma spraying
KW - Sublayer numbers
UR - https://www.scopus.com/pages/publications/85141893225
U2 - 10.1016/j.jmst.2022.09.013
DO - 10.1016/j.jmst.2022.09.013
M3 - 文章
AN - SCOPUS:85141893225
SN - 1005-0302
VL - 140
SP - 153
EP - 162
JO - Journal of Materials Science and Technology
JF - Journal of Materials Science and Technology
ER -