TY - JOUR
T1 - Region-specific ablation mechanisms and performance enhancement via Ta addition in (Hf,Zr)C-based ultra-high temperature ceramics
AU - Li, Yuxin
AU - Li, Jingtong
AU - Li, Tao
AU - Wang, Pei
AU - Zhou, Fan
AU - Zhao, Qiqi
AU - Liu, Huiqun
AU - Teng, Zhen
AU - Xue, Wei
AU - Zhang, Yulei
N1 - Publisher Copyright:
© 2026 Elsevier Ltd
PY - 2026/11
Y1 - 2026/11
N2 - Developing conventional single-component ultra-high temperature ceramics (UHTCs), such as HfC, ZrC, and TaC, with reliable ablation resistance above 2100 °C remains challenging, primarily because of phase-transition-induced cracking and the limited stability of the oxide layer. To address these limitations, bulk (Hf1/2Zr1/2)C and (Hf1/3Zr1/3Ta1/3)C solid-solution ceramics were fabricated by spark plasma sintering (SPS), and the region-specific ablation behavior was systematically investigated through experiments and finite element simulations. The results demonstrate that Ta addition plays a critical role in regulating oxidation and erosion in different ablation regions, thereby improving the ablation resistance of (Hf,Zr)C. In the central region, Ta2O5 reacts with (Hf,Zr)O2 to form Hf6Ta2O17/TaZr2.75O8 solid solutions, which suppress the phase transformation of (Hf,Zr)O2 and promote defect healing through liquid-phase Ta2O5. In the transition region, molten Ta2O5 redistributes along the direction of surface shear flow. In the edge region, the lower surface temperature and reduced thermal stress contribute to greater structural stability. These findings reveal pronounced regional differences in ablation mechanisms and clarify the effect of Ta in regulating oxidation and erosion. This work provides new insights into compositional design strategies for UHTCs intended for service above 2100 °C.
AB - Developing conventional single-component ultra-high temperature ceramics (UHTCs), such as HfC, ZrC, and TaC, with reliable ablation resistance above 2100 °C remains challenging, primarily because of phase-transition-induced cracking and the limited stability of the oxide layer. To address these limitations, bulk (Hf1/2Zr1/2)C and (Hf1/3Zr1/3Ta1/3)C solid-solution ceramics were fabricated by spark plasma sintering (SPS), and the region-specific ablation behavior was systematically investigated through experiments and finite element simulations. The results demonstrate that Ta addition plays a critical role in regulating oxidation and erosion in different ablation regions, thereby improving the ablation resistance of (Hf,Zr)C. In the central region, Ta2O5 reacts with (Hf,Zr)O2 to form Hf6Ta2O17/TaZr2.75O8 solid solutions, which suppress the phase transformation of (Hf,Zr)O2 and promote defect healing through liquid-phase Ta2O5. In the transition region, molten Ta2O5 redistributes along the direction of surface shear flow. In the edge region, the lower surface temperature and reduced thermal stress contribute to greater structural stability. These findings reveal pronounced regional differences in ablation mechanisms and clarify the effect of Ta in regulating oxidation and erosion. This work provides new insights into compositional design strategies for UHTCs intended for service above 2100 °C.
KW - (HfZrTa)C bulk ceramics
KW - Region-specific ablation mechanisms
KW - Spark plasma sintering
KW - Ultra-high temperature ceramics
UR - https://www.scopus.com/pages/publications/105050608053
U2 - 10.1016/j.corsci.2026.114205
DO - 10.1016/j.corsci.2026.114205
M3 - 文章
AN - SCOPUS:105050608053
SN - 0010-938X
VL - 272
JO - Corrosion Science
JF - Corrosion Science
M1 - 114205
ER -