TY - JOUR
T1 - Reaction time governs phase selection and fracture path transition during transient interfacial resistance brazing of Ti3AlC2 to Cu
AU - Chen, Haiyan
AU - Xiang, Jiabao
AU - Song, Xiaoguo
AU - Pan, Zhaoyi
AU - Wang, Peng
AU - Huang, Xi
AU - Cao, Jian
AU - Wang, Pengcheng
AU - Li, Wenya
N1 - Publisher Copyright:
© 2026 Elsevier Ltd.
PY - 2027/3
Y1 - 2027/3
N2 - Prolonged liquid exposure in AgCu brazing degrades Ti3AlC2, but its role in phase selection and fracture remains unclear. Transient interfacial resistance brazing (TIRB) and vacuum brazing (VB) were compared using identical materials. Under TIRB, a 70 s cycle peaking at 910 °C produced Cu-enriched and ceramic reaction zones of 480 ± 5 µm and 115 ± 4 µm, a ratio of 4.17. Under VB at 860 °C, the ratio was 0.39, with widths of 86 ± 3 µm and 221 ± 5 µm. TIRB yielded Ti3(Al, Cu)C2 with TiC confined to a thin interfacial layer, whereas VB yielded Ti2(Al, Cu)C and AlCu2Ti with broader Ti and Al redistribution. The hardness ratio between metallic constituents fell from 5.5 to 1.8. Fracture shifted from the ceramic reaction zone to the Cu-enriched zone, while shear strength rose from 116 ± 2–143 ± 5 MPa. Reaction duration is thus a kinetic parameter for regulating phase constitution and fracture location in Ti3AlC2/Cu joints.
AB - Prolonged liquid exposure in AgCu brazing degrades Ti3AlC2, but its role in phase selection and fracture remains unclear. Transient interfacial resistance brazing (TIRB) and vacuum brazing (VB) were compared using identical materials. Under TIRB, a 70 s cycle peaking at 910 °C produced Cu-enriched and ceramic reaction zones of 480 ± 5 µm and 115 ± 4 µm, a ratio of 4.17. Under VB at 860 °C, the ratio was 0.39, with widths of 86 ± 3 µm and 221 ± 5 µm. TIRB yielded Ti3(Al, Cu)C2 with TiC confined to a thin interfacial layer, whereas VB yielded Ti2(Al, Cu)C and AlCu2Ti with broader Ti and Al redistribution. The hardness ratio between metallic constituents fell from 5.5 to 1.8. Fracture shifted from the ceramic reaction zone to the Cu-enriched zone, while shear strength rose from 116 ± 2–143 ± 5 MPa. Reaction duration is thus a kinetic parameter for regulating phase constitution and fracture location in Ti3AlC2/Cu joints.
KW - Fracture-path transition
KW - Interfacial phase selection
KW - Reaction-time-scale control
KW - TiAlC/Cu Joint
KW - Transient interfacial resistance brazing
UR - https://www.scopus.com/pages/publications/105052042459
U2 - 10.1016/j.jeurceramsoc.2026.118924
DO - 10.1016/j.jeurceramsoc.2026.118924
M3 - 文章
AN - SCOPUS:105052042459
SN - 0955-2219
VL - 47
JO - Journal of the European Ceramic Society
JF - Journal of the European Ceramic Society
IS - 3
M1 - 118924
ER -