The undercooling dependence of the solidification mechanism was systematically explored by the electrostatic levitation (ESL) facility. During the experiments, the maximum undercooling reached up to 406 K (0.26 TL) and the growth velocity of the primary TiNi phase was in-situ determined at various undercoolings. At the initial increase of alloy undercooling, the value of growth velocity sluggishly rose followed by a power function. In this case, the primary TiNi phase preferentially developed as the equiaxed dendrite, then the remnant liquid participated as Ti2Ni and α-Ti phases on the grain boundary. Once the undercooling exceeded the critical value of 350 K, the growth velocity of the primary phase displayed a sharply increase tendency. Meanwhile, the TEM results demonstrated that the precipitation of the intermetallic Ti2Ni compound was gradually restrained during the rapid solidification and the R-phase existing in the TiNi matrix at large undercooling implied that the martensitic transformation was incomplete.
| 源语言 | 英语 |
|---|---|
| 页(从-至) | 82-89 |
| 页数 | 8 |
| 期刊 | Journal of Materials Science and Technology |
| 卷 | 77 |
| DOI | |
| 出版状态 | 已出版 - 30 6月 2021 |
指纹
探究 'Rapid Growth of TiNi intermetallic compound within undercooled Ti50Ni50 alloy under electrostatic levitation condition' 的科研主题。它们共同构成独一无二的指纹。引用此
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver