TY - JOUR
T1 - Process Optimization, Microstructure and Mechanical Properties of SiC + TiB2/AlSi10Mg Composites Fabricated by Laser-Directed Energy Deposition
AU - Zhang, Xin
AU - Zhang, Siyu
AU - Peng, Yijie
AU - Geng, Long
AU - Kang, Chennuo
AU - Feng, Zhe
AU - Fan, Wei
AU - Tan, Hua
AU - Lin, Xin
N1 - Publisher Copyright:
© 2025 by the authors.
PY - 2025/12
Y1 - 2025/12
N2 - In this study, TiB2/AlSi10Mg, 2 wt.% SiC + TiB2/AlSi10Mg, and 5 wt.% SiC + TiB2/AlSi10Mg composite powders were prepared via high-energy ball milling. For the first time, TiB2 and SiC hybrid particle-reinforced aluminum matrix composites (AMCs) were fabricated using the Laser-Directed Energy Deposition (LDED) technique. The effects of processing parameters on the microstructure evolution and mechanical properties were systematically investigated. Using areal energy density as the main variable, the experiments combined microstructural characterization and mechanical testing to elucidate the underlying strengthening and failure mechanisms. The results indicate that both 2 wt.% and 5 wt.% SiC + TiB2/AlSi10Mg composites exhibit excellent formability, achieving a relative density of 98.9%. However, the addition of 5 wt.% SiC leads to the formation of brittle Al4C3 and TiC phases within the matrix. Compared with the LDED-fabricated AlSi10Mg alloy, the tensile strength of the TiB2/AlSi10Mg composite increased by 21.4%. In contrast, the tensile strengths of the 2 wt.% and 5 wt.% SiC + TiB2/AlSi10Mg composites decreased by 3.7% and 2.6%, respectively, mainly due to SiC particle agglomeration and the consumption of TiB2 particles caused by TiC formation. Nevertheless, their elastic moduli were enhanced by 9% and 16.3%, respectively. Fracture analysis revealed that the composites predominantly exhibited ductile fracture characteristics. However, pores larger than 10 μm and SiC/TiB2 clusters acted as crack initiation sites, inducing stress concentration and promoting the propagation of secondary cracks.
AB - In this study, TiB2/AlSi10Mg, 2 wt.% SiC + TiB2/AlSi10Mg, and 5 wt.% SiC + TiB2/AlSi10Mg composite powders were prepared via high-energy ball milling. For the first time, TiB2 and SiC hybrid particle-reinforced aluminum matrix composites (AMCs) were fabricated using the Laser-Directed Energy Deposition (LDED) technique. The effects of processing parameters on the microstructure evolution and mechanical properties were systematically investigated. Using areal energy density as the main variable, the experiments combined microstructural characterization and mechanical testing to elucidate the underlying strengthening and failure mechanisms. The results indicate that both 2 wt.% and 5 wt.% SiC + TiB2/AlSi10Mg composites exhibit excellent formability, achieving a relative density of 98.9%. However, the addition of 5 wt.% SiC leads to the formation of brittle Al4C3 and TiC phases within the matrix. Compared with the LDED-fabricated AlSi10Mg alloy, the tensile strength of the TiB2/AlSi10Mg composite increased by 21.4%. In contrast, the tensile strengths of the 2 wt.% and 5 wt.% SiC + TiB2/AlSi10Mg composites decreased by 3.7% and 2.6%, respectively, mainly due to SiC particle agglomeration and the consumption of TiB2 particles caused by TiC formation. Nevertheless, their elastic moduli were enhanced by 9% and 16.3%, respectively. Fracture analysis revealed that the composites predominantly exhibited ductile fracture characteristics. However, pores larger than 10 μm and SiC/TiB2 clusters acted as crack initiation sites, inducing stress concentration and promoting the propagation of secondary cracks.
KW - SiC + TiB/AlSi10Mg
KW - additive manufacturing
KW - mechanical properties
KW - microstructural evolution
KW - process characteristics
UR - https://www.scopus.com/pages/publications/105025805674
U2 - 10.3390/jmmp9120404
DO - 10.3390/jmmp9120404
M3 - 文章
AN - SCOPUS:105025805674
SN - 2504-4494
VL - 9
JO - Journal of Manufacturing and Materials Processing
JF - Journal of Manufacturing and Materials Processing
IS - 12
M1 - 404
ER -