Pyrocarbons were deposited on SiC fibers from the gaseous mixture of C3H6 and N2 at temperatures range from 800°C to 1200°C. The variations of deposition rate and surface morphology along with the changes of temperature, total pressure and PN2/PC3H6 have been studied. The results show that pyrocarbons could hardly be obtained under the condition where the temperature and total pressure were below 800°C and 1 kPa, respectively. Deposition rate increases and the morphology of pyrocarbons alters from uniform depositions to uneven ones with the increasing of the temperature and total pressure. Low ratio of PN2/PC3H6 leads to pyrocarbon granulation products. Compact as well as even pyrocarbons were obtained when deposition temperature was 1000°C, total pressure 10 kPa and PN2/PC3H6 2:1 approximately. The changes of processing parameters could result in the changes of reaction thermodynamics and kinetics, which in turn is the main reason for the changes of the surface morphology.

源语言英语
页(从-至)690-692
页数3
期刊Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering
36
SUPPL. 2
出版状态已出版 - 8月 2007

指纹

探究 'Preparation of pyrocarbon coatings on SiCF' 的科研主题。它们共同构成独一无二的指纹。

引用此