The materials and preparation of multilayer for carbon-carbon (C/C) composite with Si-W outer layer, SiC barrier layer and SiC transition layer were studied to obtain long-lived and anti-oxidized coating. The technology of preparation for composite coating was determined. The transition SiC layer was prepared by siliconization at 1450 °C for 15 minutes, the dense SiC barrier layer was prepared by normal and changed temperature CVD (chemical vapor deposition) at 1100-1250 °C for 30 minutes, the pure Si-W layer was prepared by liquid reaction method at 1500 °C for 10 minutes. The experimental analysis was performed by scan electron microscopy and the effects of technological parameters on anti-oxidized performances of the composite were studied.
| 源语言 | 英语 |
|---|---|
| 页(从-至) | 129-132 |
| 页数 | 4 |
| 期刊 | Xibei Gongye Daxue Xuebao/Journal of Northwestern Polytechnical University |
| 卷 | 16 |
| 期 | 1 |
| 出版状态 | 已出版 - 1998 |
学术指纹
探究 'Preparation of a multi-layer coating for carbon-carbon composites' 的科研主题。它们共同构成独一无二的学术指纹。引用此
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver