TY - JOUR
T1 - Preparation and properties of green crosslinked styrene butadiene rubber with poly (Malic Acid)
AU - Yin, Changjie
AU - Wu, Yibo
AU - Li, Huimin
AU - Yin, Dezhong
AU - Zhang, Qiuyu
N1 - Publisher Copyright:
© The Polymer Society, Taipei 2026.
PY - 2026/9
Y1 - 2026/9
N2 - Nowadays, the most widely used vulcanization system for industrial rubber products is the traditional sulfur vulcanization system, which releases harmful gases and makes unsustainability for the development of rubber industry. Herein. In this study, the novel poly(Malic Acid) (PMA) is prepared by direct polymerization, the structure of PMA was confirmed by FTIR and 1HNMR, weight average molecular thermal stability of PMA is 4860 g/mol and 214 °C. Based on prepared EESBR with (Epoxidized emulsion styrene butadiene rubber) different epoxidized degrees, it was cured by PMA. It was found that PMA cured EESBR exhibits typical vulcanization behavior, with the increase of PMA addition, the crosslinking density increased to 9.39 × 10− 4 mol/cm3, and the tensile strength of PMA/EESBR gradually increased to 2.82 MPa, maximum torque (MH) can reach to 4.70 N*m. The value of tanδ at 60 °C and 0 °C are 0.0215 and 0.8625 respectively, exhibiting high wet skid resistance and low rolling resistance as a green tire tread. After one reprocessing properties of EESBR/PMA, the recovery rate is only 50%, it indicates that the crosslinked bonds in EESBR/PMA have not only dynamic hydroxyl ester bonds, but also irreversible ether bonds.
AB - Nowadays, the most widely used vulcanization system for industrial rubber products is the traditional sulfur vulcanization system, which releases harmful gases and makes unsustainability for the development of rubber industry. Herein. In this study, the novel poly(Malic Acid) (PMA) is prepared by direct polymerization, the structure of PMA was confirmed by FTIR and 1HNMR, weight average molecular thermal stability of PMA is 4860 g/mol and 214 °C. Based on prepared EESBR with (Epoxidized emulsion styrene butadiene rubber) different epoxidized degrees, it was cured by PMA. It was found that PMA cured EESBR exhibits typical vulcanization behavior, with the increase of PMA addition, the crosslinking density increased to 9.39 × 10− 4 mol/cm3, and the tensile strength of PMA/EESBR gradually increased to 2.82 MPa, maximum torque (MH) can reach to 4.70 N*m. The value of tanδ at 60 °C and 0 °C are 0.0215 and 0.8625 respectively, exhibiting high wet skid resistance and low rolling resistance as a green tire tread. After one reprocessing properties of EESBR/PMA, the recovery rate is only 50%, it indicates that the crosslinked bonds in EESBR/PMA have not only dynamic hydroxyl ester bonds, but also irreversible ether bonds.
KW - Green crosslinked
KW - Poly malic acid
KW - Rubber
KW - β-hydroxy ester bonds
UR - https://www.scopus.com/pages/publications/105048770242
U2 - 10.1007/s10965-026-05098-9
DO - 10.1007/s10965-026-05098-9
M3 - 文章
AN - SCOPUS:105048770242
SN - 1022-9760
VL - 33
JO - Journal of Polymer Research
JF - Journal of Polymer Research
IS - 9
M1 - 375
ER -