TY - JOUR
T1 - Preparation and long-term ablation behavior of Cf-reinforced ZrC-SiC coated C/C-ZrC-SiC composite
AU - Zhong, Lei
AU - Guo, Lingjun
AU - Wang, Chuanyun
AU - Liu, Ningkun
AU - shen, Qingliang
AU - Li, Hejun
AU - Li, Yunyu
N1 - Publisher Copyright:
© 2023 Elsevier Ltd
PY - 2024/2
Y1 - 2024/2
N2 - To improve the long-term ablation resistance of the C/C composite, the Cf-reinforced ZrC-SiC coated C/C-ZrC-SiC composite is fabricated by thermal gradient chemical vapor infiltration (TGCVI) technology and the subsequent polymer infiltration and pyrolysis (PIP) process. The coating shares the same carbon fiber felt with the matrix, which can strengthen the bond between the coating and the matrix. Results show that the composite has excellent long-term anti-ablation performance (the linear ablation rate of the composite is −0.64 µm/s after ablated for 120 s (3 × 40 s), and the coating can withstand ablation for 160 s (4 × 40 s) without destruction). With the reinforcement of carbon fibers, the coating is peeled layer by layer rather than destructed in the whole coating, and the coating still works in the subsequent ablation cycles (the linear ablation rate of the composite is 2.40 µm/s after ablated for 280 s (7 × 40 s)).
AB - To improve the long-term ablation resistance of the C/C composite, the Cf-reinforced ZrC-SiC coated C/C-ZrC-SiC composite is fabricated by thermal gradient chemical vapor infiltration (TGCVI) technology and the subsequent polymer infiltration and pyrolysis (PIP) process. The coating shares the same carbon fiber felt with the matrix, which can strengthen the bond between the coating and the matrix. Results show that the composite has excellent long-term anti-ablation performance (the linear ablation rate of the composite is −0.64 µm/s after ablated for 120 s (3 × 40 s), and the coating can withstand ablation for 160 s (4 × 40 s) without destruction). With the reinforcement of carbon fibers, the coating is peeled layer by layer rather than destructed in the whole coating, and the coating still works in the subsequent ablation cycles (the linear ablation rate of the composite is 2.40 µm/s after ablated for 280 s (7 × 40 s)).
KW - C-reinforced ZrC-SiC coating
KW - Cycle ablation
KW - Finite Element Analysis (FEA)
KW - Thermal gradient chemical vapour infiltration (TGCVI)
UR - https://www.scopus.com/pages/publications/85171892991
U2 - 10.1016/j.jeurceramsoc.2023.09.037
DO - 10.1016/j.jeurceramsoc.2023.09.037
M3 - 文章
AN - SCOPUS:85171892991
SN - 0955-2219
VL - 44
SP - 693
EP - 704