TY - JOUR
T1 - Preparation and ablation properties of the SiC/ZrB2-SiC gradient ceramic coating on C/C-ZrC-SiC composites
AU - Zhang, Guangxi
AU - Tian, Xinfa
AU - Zhang, Haoqian
AU - Xiao, Jinyou
AU - Zhang, Pengfei
AU - Hou, Xiao
N1 - Publisher Copyright:
© 2025 Elsevier Ltd and Techna Group S.r.l. All rights are reserved, including those for text and data mining, AI training, and similar technologies.
PY - 2025/11
Y1 - 2025/11
N2 - The SiC/ZrB2-SiC gradient ceramic (S/ZS) coating and ZrB2-SiC ceramic (ZS) coating were prepared via slurry brushing and liquid silicon infiltration methods. The microstructure evolution and ablation behaviors of the S/ZS and ZS coatings were systematically investigated and compared. The S/ZS coating and matrix were closely bonded due to the formation of SiC at the interfaces. Meanwhile, the ingredient gradient from the SiC transition coating reduced the coefficient of thermal expansion (CTE) mismatch between the matrix and the outer ceramic coating. Therefore, the adhesion strength of the S/ZS coating was 38.48 % higher than that of the ZS coating. After 90 s of ablation, the ZS coating exhibited obvious peeling, while the S/ZS coating still remained intact. Correspondingly, the mass and linear ablation rates of the ZS coating were 709.09 % and 274 % higher than those of the S/ZS coating, respectively. In this work, the SiC transition coating could improve the structural integrity of the oxide layer and enhance the ablation performance of the coating.
AB - The SiC/ZrB2-SiC gradient ceramic (S/ZS) coating and ZrB2-SiC ceramic (ZS) coating were prepared via slurry brushing and liquid silicon infiltration methods. The microstructure evolution and ablation behaviors of the S/ZS and ZS coatings were systematically investigated and compared. The S/ZS coating and matrix were closely bonded due to the formation of SiC at the interfaces. Meanwhile, the ingredient gradient from the SiC transition coating reduced the coefficient of thermal expansion (CTE) mismatch between the matrix and the outer ceramic coating. Therefore, the adhesion strength of the S/ZS coating was 38.48 % higher than that of the ZS coating. After 90 s of ablation, the ZS coating exhibited obvious peeling, while the S/ZS coating still remained intact. Correspondingly, the mass and linear ablation rates of the ZS coating were 709.09 % and 274 % higher than those of the S/ZS coating, respectively. In this work, the SiC transition coating could improve the structural integrity of the oxide layer and enhance the ablation performance of the coating.
KW - Ablation behavior
KW - C/C-ZrC-SiC composite
KW - Liquid silicon infiltration
KW - SiC/ZrB-SiC gradient ceramic coating
KW - Slurry brushing
UR - https://www.scopus.com/pages/publications/105013466787
U2 - 10.1016/j.ceramint.2025.08.077
DO - 10.1016/j.ceramint.2025.08.077
M3 - 文章
AN - SCOPUS:105013466787
SN - 0272-8842
VL - 51
SP - 48201
EP - 48208
JO - Ceramics International
JF - Ceramics International
IS - 26
ER -