This study exhibits the possibility of using an artificial neural network (ANN) to model the mechanical behavior of wire arc additive manufacturing (WAAM) for Inconel 625. For this reason, tensile tests of Inconel 625 superalloy as-built (AB) samples and samples after heat treatment at 1200 °C (HT-1200) by WAAM were performed. For the HT-1200 samples, the yield stress decreased, and the elongation increased significantly due to grain refinement and the formation of annealed twins. A new hybrid model combining a swarm intelligence optimization algorithm with a back propagation neural network (BPNN) was developed to simulate the flow behavior of the superalloy. Compared with other hybrid BPNN models that have been reported, the proposed BPNN model is in better agreement with the experimental data and provides a better description of the flow stress of the Inconel 625 superalloy. The excellent predictive ability of the model may be attributed to the optimization of the weights and thresholds of the BPNN, which obtains the optimal global solution in the search space more efficiently.
| 源语言 | 英语 |
|---|---|
| 文章编号 | 3240 |
| 期刊 | Applied Sciences (Switzerland) |
| 卷 | 14 |
| 期 | 8 |
| DOI | |
| 出版状态 | 已出版 - 4月 2024 |
指纹
探究 'Prediction of Tensile Properties in Inconel 625 Superalloy Fabricated by Wire Arc Additive Manufacturing Using Improved Artificial Neural Network' 的科研主题。它们共同构成独一无二的指纹。引用此
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver