TY - JOUR
T1 - Plasma ablation behavior of VC modified C/C-(Hf, Zr)C composites prepared by precursor infiltration and pyrolysis
AU - Wang, Shenghong
AU - He, Qinchuan
AU - Wang, Yiqun
AU - Fan, Congmin
AU - Yin, Xuemin
N1 - Publisher Copyright:
© 2026 Elsevier Ltd.
PY - 2027/3
Y1 - 2027/3
N2 - VC modified C/C-(Hf, Zr)C composites with different VC contents were prepared by a precursor infiltration and pyrolysis method, and their plasma ablation behavior was investigated. The results show that an appropriate amount of VC significantly enhances the ablation resistance. The 12 wt% sample exhibited the lowest mass and linear ablation rates after 90 s of ablation, which were 0.43 mg/s and 4.58 μm/s, respectively. During ablation, (Hf, Zr)C is preferentially oxidized to form a high-melting (Hf, Zr)O2 framework, which provides the main structural support for the protective oxide layers. Meanwhile, VC oxidation produces V-containing oxides. In the ablation center, these oxides tend to volatilize and consume heat, while in relatively lower-temperature regions they can exist as a liquid phase and assist in sealing pores and microcracks. However, excessive VC generates too much volatile V-containing oxide, weakens the continuity of the oxide layer, and eventually deteriorates the ablation resistance.
AB - VC modified C/C-(Hf, Zr)C composites with different VC contents were prepared by a precursor infiltration and pyrolysis method, and their plasma ablation behavior was investigated. The results show that an appropriate amount of VC significantly enhances the ablation resistance. The 12 wt% sample exhibited the lowest mass and linear ablation rates after 90 s of ablation, which were 0.43 mg/s and 4.58 μm/s, respectively. During ablation, (Hf, Zr)C is preferentially oxidized to form a high-melting (Hf, Zr)O2 framework, which provides the main structural support for the protective oxide layers. Meanwhile, VC oxidation produces V-containing oxides. In the ablation center, these oxides tend to volatilize and consume heat, while in relatively lower-temperature regions they can exist as a liquid phase and assist in sealing pores and microcracks. However, excessive VC generates too much volatile V-containing oxide, weakens the continuity of the oxide layer, and eventually deteriorates the ablation resistance.
KW - (Hf, Zr)C
KW - C/C composites
KW - Modification
KW - Plasma ablation
KW - VC
UR - https://www.scopus.com/pages/publications/105052495755
U2 - 10.1016/j.jeurceramsoc.2026.118943
DO - 10.1016/j.jeurceramsoc.2026.118943
M3 - 文章
AN - SCOPUS:105052495755
SN - 0955-2219
VL - 47
JO - Journal of the European Ceramic Society
JF - Journal of the European Ceramic Society
IS - 3
M1 - 118943
ER -