摘要
Directional solidification of LaB6-ZrB2, by use of an electron beam heating technique, yielded oriented ZrB2 fibers in a LaB6 matrix. The average diameter of the ZrB2 fibers was ≃0.2-1.2 μm, with fiber lengths up to 100 μm. Primary platelike LaB6 dendrites formed upon the solidification of an ingot with a composition of LaB6-18 wt% ZrB2. LaB6 was the first phase to nucleate when eutectic growth occurred, and ZrB2 showed nonfaceted growth. For the ingot solidified with planar growth the orientation relations of the phases were as follows: growth direction, [001]LaB6∥[00.1]ZrB2; interfacial plane, (11.0)LaB6∥(11.0)ZrB2.
| 源语言 | 英语 |
|---|---|
| 页(从-至) | 237-240 |
| 页数 | 4 |
| 期刊 | Journal of the American Ceramic Society |
| 卷 | 81 |
| 期 | 1 |
| DOI | |
| 出版状态 | 已出版 - 1月 1998 |
指纹
探究 'Oriented structure and crystallography of directionally solidified LaB6-ZrB2 eutectic' 的科研主题。它们共同构成独一无二的指纹。引用此