On the poisoning effect of O 2 and N 2 for the Zr 0.9Ti 0.1V 2 hydrogen storage alloy

  • Northwestern Polytechnical University Xian

科研成果: 期刊稿件文章同行评审

48 引用 (Scopus)

摘要

Homogeneously annealed Zr 0.9Ti 0.1V 2 samples are firstly exposed to contamination gases of O 2 and N 2 for 30, 60 and 180 s at the ambient temperature, respectively. Hydrogen absorption properties are examined after poisoning and regeneration. The compositions and valence in the surface and sub-surface are investigated by X-ray photoelectron spectroscopy (XPS). The hydrogen absorption capacity of the alloy has been almost entirely degraded by the oxygen poisoning. After the regeneration, the oxygen-poisoned sample can hardly absorb hydrogen while the nitrogen-poisoned sample re-obtains the hydrogen absorption capacity with the value as 2.85 H A -1 (molar ratio of hydrogen to alloy). The activation temperature of the oxygen-poisoned sample is ∼100 K higher than the value of the un-poisoned one. With the help of ion etching, it is found the thickness of the passivated surface layer of the oxygen-poisoned sample was ∼58 nm. However, the thickness of the passivated surface layer of the un-poisoned sample is only ∼36 nm. That is the reason why the oxygen-poisoned sample cannot renew the hydrogen absorption capacity under the same regeneration conditions as in the un-poisoned one.

源语言英语
页(从-至)217-224
页数8
期刊Journal of Power Sources
202
DOI
出版状态已出版 - 15 3月 2012

联合国可持续发展目标

此成果有助于实现下列可持续发展目标:

  1. 可持续发展目标 7 - 经济适用的清洁能源
    可持续发展目标 7 经济适用的清洁能源

学术指纹

探究 'On the poisoning effect of O 2 and N 2 for the Zr 0.9Ti 0.1V 2 hydrogen storage alloy' 的科研主题。它们共同构成独一无二的学术指纹。

引用此