TY - JOUR
T1 - Nanostructured hypoeutectic Fe-B alloy prepared by a self-propagating high temperature synthesis combining a rapid cooling technique
AU - Fu, Licai
AU - Yang, Jun
AU - Bi, Qinling
AU - Liu, Weimin
PY - 2009/1
Y1 - 2009/1
N2 - We have successfully synthesized bulk nanostructured Fe 94.3B 5.7 alloy using the one-step approach of a self-propagating high temperature synthesis (SHS) combining a rapid cooling technique. This method is convenient, low in cost, and capable of being scaled up for processing the bulk nanostructured materials. The solidification microstructure is composed of a relatively coarse, uniformly distributed dendriteto a nanostructured eutectic matrix with α-Fe(B) and t-Fe 2B phases. The fine eutectic structure is disorganized, and the precipitation Fe 2B is found in the α-Fe(B) phase of the eutectic. The dendrite phase has the t-Fe 2B structure rather than α-Fe(B) in the Fe 94.3B 5.7 alloy, because the growth velocity of t-Fe 2B is faster than that of the α-Fe with the deeply super-cooling degree. The coercivity (Hc) and saturation magnetization (Ms) values of the Fe 94.3B 5.7 alloy are 11 A/m and 1.74T, respectively. Moreover, the Fe 94.3B 5.7 alloy yields at 1430 MPa and fractures at 1710 MPa with a large ductility of 19.8% at compressive test.
AB - We have successfully synthesized bulk nanostructured Fe 94.3B 5.7 alloy using the one-step approach of a self-propagating high temperature synthesis (SHS) combining a rapid cooling technique. This method is convenient, low in cost, and capable of being scaled up for processing the bulk nanostructured materials. The solidification microstructure is composed of a relatively coarse, uniformly distributed dendriteto a nanostructured eutectic matrix with α-Fe(B) and t-Fe 2B phases. The fine eutectic structure is disorganized, and the precipitation Fe 2B is found in the α-Fe(B) phase of the eutectic. The dendrite phase has the t-Fe 2B structure rather than α-Fe(B) in the Fe 94.3B 5.7 alloy, because the growth velocity of t-Fe 2B is faster than that of the α-Fe with the deeply super-cooling degree. The coercivity (Hc) and saturation magnetization (Ms) values of the Fe 94.3B 5.7 alloy are 11 A/m and 1.74T, respectively. Moreover, the Fe 94.3B 5.7 alloy yields at 1430 MPa and fractures at 1710 MPa with a large ductility of 19.8% at compressive test.
KW - Fe B alloy
KW - Mechanical behavior
KW - Nanostructured eutectic
KW - Self-propagating high temperature synthesis (SHS)
KW - Soft magnetic performance
UR - https://www.scopus.com/pages/publications/58549091728
U2 - 10.1007/s11671-008-9195-4
DO - 10.1007/s11671-008-9195-4
M3 - 文章
AN - SCOPUS:58549091728
SN - 1931-7573
VL - 4
SP - 11
EP - 16
JO - Nanoscale Research Letters
JF - Nanoscale Research Letters
IS - 1
ER -