TY - JOUR
T1 - Microwave-hydrothermal method post-treatment of sprayed Ca-P coating
AU - Su, Yangyang
AU - Li, Kezhi
AU - Zhu, Xiaofei
AU - Wang, Changcong
AU - Zhang, Yunpeng
N1 - Publisher Copyright:
© 2018 Elsevier Ltd and Techna Group S.r.l.
PY - 2019/1
Y1 - 2019/1
N2 - Supersonic atmospheric plasma sprayed (SAPS) calcium phosphate (Ca-P) coating is post-processed by microwave-hydrothermal (MH) method for the reduction of the surface defects in our previous work. During the MH process, ethylenediaminetetraacetic disodium salt (Na2EDTA) as complexing agent is added during the MH reaction, while controlling the pH values, to achieve the purpose of grain refinement and decrease the surface defects, and enhance the corrosion resistance of the sprayed Ca-P coating. Afterward, surface morphologies, element and phase composition of the coating, chemical groups, surface roughness, porosity, bioactivity and corrosion resistance are all studied. The results show that the addition of Na2EDTA and the adjustment of pH value during MH treatment do have a positive effect on grain refinement, and improvement the bioactivity and corrosion resistance of the sprayed Ca-P coating. Expressly, their corresponding corrosion potential are − 0.1105 ± 0.0025, − 0.1072 ± 0.0012 and − 0.3021 ± 0.0021 V according to the corrosion current density 2.19 × 10−6, 1.89 × 10−5and 1.71 × 10−5 A/cm2, respectively.
AB - Supersonic atmospheric plasma sprayed (SAPS) calcium phosphate (Ca-P) coating is post-processed by microwave-hydrothermal (MH) method for the reduction of the surface defects in our previous work. During the MH process, ethylenediaminetetraacetic disodium salt (Na2EDTA) as complexing agent is added during the MH reaction, while controlling the pH values, to achieve the purpose of grain refinement and decrease the surface defects, and enhance the corrosion resistance of the sprayed Ca-P coating. Afterward, surface morphologies, element and phase composition of the coating, chemical groups, surface roughness, porosity, bioactivity and corrosion resistance are all studied. The results show that the addition of Na2EDTA and the adjustment of pH value during MH treatment do have a positive effect on grain refinement, and improvement the bioactivity and corrosion resistance of the sprayed Ca-P coating. Expressly, their corresponding corrosion potential are − 0.1105 ± 0.0025, − 0.1072 ± 0.0012 and − 0.3021 ± 0.0021 V according to the corrosion current density 2.19 × 10−6, 1.89 × 10−5and 1.71 × 10−5 A/cm2, respectively.
KW - Calcium phosphate coating
KW - Ethylenediaminetetraacetic disodium salt
KW - Grain refinement
KW - Microwave-hydrothermal
KW - Supersonic atmospheric plasma spray
UR - https://www.scopus.com/pages/publications/85054436796
U2 - 10.1016/j.ceramint.2018.09.258
DO - 10.1016/j.ceramint.2018.09.258
M3 - 文章
AN - SCOPUS:85054436796
SN - 0272-8842
VL - 45
SP - 874
EP - 884
JO - Ceramics International
JF - Ceramics International
IS - 1