TY - JOUR
T1 - Microstructure, mechanical properties and high-throughput characterization of directionally solidified B4C-TiB2 and B4C-SiC eutectic ceramics
AU - Ren, Qun
AU - Su, Haijun
AU - Yang, Xirong
AU - Cui, Chunjuan
AU - Wang, Yenan
AU - Han, Yuyang
AU - Yang, Xinyu
N1 - Publisher Copyright:
© 2026 Published by Elsevier Ltd.
PY - 2027/1
Y1 - 2027/1
N2 - B4C-TiB2 and B4C-SiC DSECs (directionally solidified eutectic ceramics) were fabricated, and their microstructures, defects, dislocations, and mechanical properties were analyzed. Furthermore, a novel high-throughput microstructure characterization method was proposed. For B4C-TiB2 eutectics, an irregular weak-faceted lamellar/rod-like microstructure was exhibited at lower solidification rates, while the coexistence of lamellar and rod-like patterns was observed with increasing solidification rates. Meanwhile, B4C-SiC eutectics showed strongly faceted growth behavior with an irregular eutectic microstructure at low solidification rates. However, at higher solidification rates, they exhibited the coexistence of irregular faceted, regular weak-faceted, rod-like, and triangular-like eutectic forms. Microhardness values (38.6 GPa and 37.8 GPa) and toughness values (3.3 MPa m1/2 and 2.5 MPa m1/2) were achieved for B4C-TiB2 and B4C-SiC specimens. Eutectic microstructure refinement and dislocation characteristics derived from KAM (kernel average misorientation) and geometrically necessary dislocation densities (GNDs) results constitute important mechanisms for hardness enhancement. A new strategy combining nanoscale metallographic polishing and white light interferometry (NMP-WLI) was proposed for the high-throughput microstructure characterization of B4C-TiB2 and B4C-SiC DSECs. Phase-dependent wear differences resulted in distinctly opposite height contrasts: B4C was higher than TiB2 in B4C-TiB2 DSECs, whereas B4C was lower than SiC in B4C-SiC DSECs.
AB - B4C-TiB2 and B4C-SiC DSECs (directionally solidified eutectic ceramics) were fabricated, and their microstructures, defects, dislocations, and mechanical properties were analyzed. Furthermore, a novel high-throughput microstructure characterization method was proposed. For B4C-TiB2 eutectics, an irregular weak-faceted lamellar/rod-like microstructure was exhibited at lower solidification rates, while the coexistence of lamellar and rod-like patterns was observed with increasing solidification rates. Meanwhile, B4C-SiC eutectics showed strongly faceted growth behavior with an irregular eutectic microstructure at low solidification rates. However, at higher solidification rates, they exhibited the coexistence of irregular faceted, regular weak-faceted, rod-like, and triangular-like eutectic forms. Microhardness values (38.6 GPa and 37.8 GPa) and toughness values (3.3 MPa m1/2 and 2.5 MPa m1/2) were achieved for B4C-TiB2 and B4C-SiC specimens. Eutectic microstructure refinement and dislocation characteristics derived from KAM (kernel average misorientation) and geometrically necessary dislocation densities (GNDs) results constitute important mechanisms for hardness enhancement. A new strategy combining nanoscale metallographic polishing and white light interferometry (NMP-WLI) was proposed for the high-throughput microstructure characterization of B4C-TiB2 and B4C-SiC DSECs. Phase-dependent wear differences resulted in distinctly opposite height contrasts: B4C was higher than TiB2 in B4C-TiB2 DSECs, whereas B4C was lower than SiC in B4C-SiC DSECs.
KW - Carbide-based eutectic ceramics
KW - High-throughput characterization
KW - Mechanical property
KW - Microstructure
KW - Optical floating zone melting (OFZM)
UR - https://www.scopus.com/pages/publications/105053807162
U2 - 10.1016/j.vacuum.2026.115882
DO - 10.1016/j.vacuum.2026.115882
M3 - 文章
AN - SCOPUS:105053807162
SN - 0042-207X
VL - 255
JO - Vacuum
JF - Vacuum
M1 - 115882
ER -