TY - JOUR
T1 - Microstructure evolution and mechanical properties of nuclear zircaloy-4 alloy fabricated by laser powder bed fusion at varying laser energy densities
AU - Zhang, Zhe
AU - Yao, Bo
AU - Feng, Zhe
AU - Hao, Zhiwei
AU - Zhou, Fan
AU - Yuan, Lukai
AU - Yang, Kuitong
AU - Li, Xiangyu
AU - Tan, Hua
AU - Lin, Xin
N1 - Publisher Copyright:
© 2025 Author(s).
PY - 2025/12/10
Y1 - 2025/12/10
N2 - Zircaloy-4 (Zr-4) is widely used in reactor fuel assemblies due to its low thermal neutron absorption properties, superior mechanical properties, and excellent corrosion resistance. Laser powder bed fusion (LPBF) technique provides potential solutions to meet the requirements of fuel assemblies, balancing complex structures with outstanding performance. Therefore, it is of great significance to investigate the microstructural characteristics and mechanical properties of Zr-4 alloy processed using LPBF through a complex solidification process. In this work, the microstructure evolution and mechanical properties of Zr-4 alloy processed under different laser volumetric energy densities (Ev) were investigated, based on an optimized process window for high relative densities of as-built parts. The LPBF-processed Zr-4 alloy exhibited a microstructure of epitaxial columnar β-grains containing highly dislocated α-laths, forming Widmanstätten and basketweave structures. As Ev increased, the width of prior β-grains and α-laths increased by 21.7% and 14.3%, respectively, while the kernel average misorientation and low-angle grain boundary fractions decreased by 40.3% and 46.8%, respectively, indicating a reduction in substructural dislocation density due to lower cooling rates. The medium-Ev specimen demonstrated superior metallurgical quality, featuring approximately 1% higher content of ~57° twin boundaries, along with grain refinement and dislocation strengthening, achieving the highest ultimate tensile strength (725.5 MPa) – approximately 70% higher than the American Society for Testing and Materials’ standard. Nevertheless, limited slip system activation in the hexagonal close-packed structure, deformation constraints from basketweave morphology, and process-induced defects, such as unmelted powder in low-Ev specimens and pores in high-Ev specimens, resulted in reduced ductility. This work provides guidance for tailoring the microstructure and achieving high mechanical properties in LPBF-processed zirconium fuel assemblies.
AB - Zircaloy-4 (Zr-4) is widely used in reactor fuel assemblies due to its low thermal neutron absorption properties, superior mechanical properties, and excellent corrosion resistance. Laser powder bed fusion (LPBF) technique provides potential solutions to meet the requirements of fuel assemblies, balancing complex structures with outstanding performance. Therefore, it is of great significance to investigate the microstructural characteristics and mechanical properties of Zr-4 alloy processed using LPBF through a complex solidification process. In this work, the microstructure evolution and mechanical properties of Zr-4 alloy processed under different laser volumetric energy densities (Ev) were investigated, based on an optimized process window for high relative densities of as-built parts. The LPBF-processed Zr-4 alloy exhibited a microstructure of epitaxial columnar β-grains containing highly dislocated α-laths, forming Widmanstätten and basketweave structures. As Ev increased, the width of prior β-grains and α-laths increased by 21.7% and 14.3%, respectively, while the kernel average misorientation and low-angle grain boundary fractions decreased by 40.3% and 46.8%, respectively, indicating a reduction in substructural dislocation density due to lower cooling rates. The medium-Ev specimen demonstrated superior metallurgical quality, featuring approximately 1% higher content of ~57° twin boundaries, along with grain refinement and dislocation strengthening, achieving the highest ultimate tensile strength (725.5 MPa) – approximately 70% higher than the American Society for Testing and Materials’ standard. Nevertheless, limited slip system activation in the hexagonal close-packed structure, deformation constraints from basketweave morphology, and process-induced defects, such as unmelted powder in low-Ev specimens and pores in high-Ev specimens, resulted in reduced ductility. This work provides guidance for tailoring the microstructure and achieving high mechanical properties in LPBF-processed zirconium fuel assemblies.
KW - Laser energy density
KW - Laser powder bed fusion
KW - Mechanical properties
KW - Microstructure
KW - Zircaloy-4
UR - https://www.scopus.com/pages/publications/105014752150
U2 - 10.36922/MSAM025220041
DO - 10.36922/MSAM025220041
M3 - 文章
AN - SCOPUS:105014752150
SN - 2810-9635
VL - 4
JO - Materials Science in Additive Manufacturing
JF - Materials Science in Additive Manufacturing
IS - 4
M1 - 025220041
ER -