TY - JOUR
T1 - Microstructure and mechanical properties of IN718 alloy fabricated by dual-laser powder bed fusion
AU - Lv, Haiyang
AU - Wang, Pei
AU - Guo, Liping
AU - Wang, Xingxing
AU - Yuan, Zhipeng
AU - Wang, Shuai
AU - Shi, Jianjun
AU - Yang, Haiou
AU - Wu, Pengyue
N1 - Publisher Copyright:
Copyright © 2026. Published by Elsevier B.V.
PY - 2026/9/1
Y1 - 2026/9/1
N2 - A highly dense IN718 alloy is fabricated via a novel synchronous dual-laser powder bed fusion (LPBF) strategy. By actively reconstructing the localized thermal history, the secondary heat input prolongs the liquid-phase lifetime, enhancing melt pool stability against defects and broadening the optimal process window. Retrospective calculations based on primary dendrite arm spacing coarsening reveal a ∼21.2% reduction in the local cooling rate. Subsequent electron backscatter diffraction (EBSD) analyses confirm this thermal modulation disrupts continuous epitaxial growth, promoting the columnar-to-equiaxed transition (CET) and mitigating crystallographic anisotropy. Furthermore, intense transverse thermal shocks induce a massive multiplication of geometrically necessary dislocations (GNDs). Driven by this enhanced work-hardening, horizontal dual-laser specimens achieve an exceptional strength-ductility synergy (yield strength: 718 ± 5 MPa, ultimate tensile strength: 1004 ± 6 MPa, elongation: 29.5%), significantly outperforming conventional single-laser benchmarks. By quantitatively decoupling these strengthening mechanisms, this study elucidates directional trade-offs between GNDs and grain boundaries, providing a tailored strategy to specifically optimize the transverse load-bearing capacity of superalloy components (e.g., turbine disks).
AB - A highly dense IN718 alloy is fabricated via a novel synchronous dual-laser powder bed fusion (LPBF) strategy. By actively reconstructing the localized thermal history, the secondary heat input prolongs the liquid-phase lifetime, enhancing melt pool stability against defects and broadening the optimal process window. Retrospective calculations based on primary dendrite arm spacing coarsening reveal a ∼21.2% reduction in the local cooling rate. Subsequent electron backscatter diffraction (EBSD) analyses confirm this thermal modulation disrupts continuous epitaxial growth, promoting the columnar-to-equiaxed transition (CET) and mitigating crystallographic anisotropy. Furthermore, intense transverse thermal shocks induce a massive multiplication of geometrically necessary dislocations (GNDs). Driven by this enhanced work-hardening, horizontal dual-laser specimens achieve an exceptional strength-ductility synergy (yield strength: 718 ± 5 MPa, ultimate tensile strength: 1004 ± 6 MPa, elongation: 29.5%), significantly outperforming conventional single-laser benchmarks. By quantitatively decoupling these strengthening mechanisms, this study elucidates directional trade-offs between GNDs and grain boundaries, providing a tailored strategy to specifically optimize the transverse load-bearing capacity of superalloy components (e.g., turbine disks).
KW - Dual-laser powder bed fusion
KW - IN718 alloy
KW - Microstructure
KW - Strengthening mechanisms
UR - https://www.scopus.com/pages/publications/105049326786
U2 - 10.1016/j.jmrt.2026.08.292
DO - 10.1016/j.jmrt.2026.08.292
M3 - 文章
AN - SCOPUS:105049326786
SN - 2238-7854
VL - 44
SP - 5580
EP - 5595
JO - Journal of Materials Research and Technology
JF - Journal of Materials Research and Technology
ER -