Mechanical behavior of C/SiC T-section under pulling load

  • Nuclear Power Institute of China
  • Northwestern Polytechnical University Xian

科研成果: 期刊稿件文章同行评审

7 引用 (Scopus)

摘要

For the C/SiC T-section structures, fabrication defects such as pores and local delaminations can be easily formed in the intersection zone which significantly affect the load bearing capacity. In this work, the mechanical behavior of C/SiC T-section under pulling load was investigated, and especially the delamination behavior was studied by introducing the cohesive zone model into the finite element modeling. It was found that for C/SiC T-section under pulling load, the maximum critical delamination load was about 1075 N in the present work, and the interface delamination was the main failure mode. It was verified that the effective interfacial strength influenced the critical delamination load, and the strain energy release affected the delamination behavior of the T-section specimen. The failure mechanisms of C/SiC T-section under pulling load depend on the interface bonding states. When the interface is well bonded, the failure mechanisms mainly include matrix stripping, matrix fracture and fiber breakage. Otherwise, only the matrix stripping can be found at the interface of the C/SiC T-section specimen.

源语言英语
页(从-至)2950-2956
页数7
期刊Journal of Materials Science and Technology
35
12
DOI
出版状态已出版 - 12月 2019

指纹

探究 'Mechanical behavior of C/SiC T-section under pulling load' 的科研主题。它们共同构成独一无二的指纹。

引用此