Low cycle fatigue behavior of single crystal superalloy with temperature gradient

  • Northwestern Polytechnical University Xian

科研成果: 期刊稿件文章同行评审

31 引用 (Scopus)

摘要

In present study, low cycle fatigue model based on rate dependent constitutive formulation with kinematic hardening and fatigue damage rule is introduced to investigate the fatigue behavior of single crystal superalloys with temperature gradient. Low cycle fatigue tests with uniform temperature and with temperature gradient are carried out to investigate the influence of temperature gradient. The microstructure reveals that the slip deformation is a principal mechanism of low cycle fatigue with temperature gradient. Complex stress experiments of low cycle fatigue are carried out to verify the life prediction rule. Bauschinger effect, ratcheting effect and fatigue damage of single crystal superalloy at different temperatures are studied. Special attention is placed on the simulation of low cycle fatigue behavior with temperature gradient. The simulation results show that the ratcheting effect at high temperature is more remarkable than that at low temperature due to the influence of temperature gradient, which results in the difference of damage evolution between high temperature zone and low temperature zone. Comparison between experiments and simulations with temperature gradient proves that the predicted model based on the damage of the second cycle is reasonable.

源语言英语
页(从-至)611-618
页数8
期刊European Journal of Mechanics, A/Solids
29
4
DOI
出版状态已出版 - 7月 2010

指纹

探究 'Low cycle fatigue behavior of single crystal superalloy with temperature gradient' 的科研主题。它们共同构成独一无二的指纹。

引用此