TY - JOUR
T1 - Long-term water-oxygen corrosion behavior and mechanism of an all-oxide Yb-Al-Si-O glass-modified Yb2Si2O7 bond coat on SiCf/SiC composites at 1400 °C
AU - Guo, Chun
AU - Chen, Yujie
AU - Ma, Yujie
AU - Li, Jianfeng
AU - Jin, Muzhen
AU - Deng, Juanli
AU - Fan, Shangwu
N1 - Publisher Copyright:
© 2026 Elsevier Ltd
PY - 2026/12
Y1 - 2026/12
N2 - The long-term water-oxygen corrosion behavior of a Yb-Al-Si-O glass-modified Yb2Si2O7 coating on SiCf/SiC composites (A-D-SS) was investigated at 1400 °C for 200 h in 50 vol% H2O-50 vol% O2. A-D-SS exhibited continuous net mass gain with a decreasing rate, governed by water-vapor incorporation, limited SiC oxidation, and Si(OH)4 volatilization. At the surface, hydrolysis and volatilization of residual YbAS glass caused Si depletion and compositional rearrangement, promoting mullite enrichment and increasing surface roughness. Independently, corrosion-induced Si loss from Yb2Si2O7 grain boundaries produced a small amount of Yb2SiO5. Within the coating, localized penetration increased porosity, but no continuous transport pathways formed. At the coating/substrate interface, limited SiC oxidation produced amorphous SiO2, while residual YbAS glass underwent local crystallization, contributing to the formation of a nanoscale multiphase interfacial structure. Overall, A-D-SS retained structural integrity and effectively restricted sustained water-oxygen penetration, demonstrating its potential as an all-oxide bond coat for SiCf/SiC composites.
AB - The long-term water-oxygen corrosion behavior of a Yb-Al-Si-O glass-modified Yb2Si2O7 coating on SiCf/SiC composites (A-D-SS) was investigated at 1400 °C for 200 h in 50 vol% H2O-50 vol% O2. A-D-SS exhibited continuous net mass gain with a decreasing rate, governed by water-vapor incorporation, limited SiC oxidation, and Si(OH)4 volatilization. At the surface, hydrolysis and volatilization of residual YbAS glass caused Si depletion and compositional rearrangement, promoting mullite enrichment and increasing surface roughness. Independently, corrosion-induced Si loss from Yb2Si2O7 grain boundaries produced a small amount of Yb2SiO5. Within the coating, localized penetration increased porosity, but no continuous transport pathways formed. At the coating/substrate interface, limited SiC oxidation produced amorphous SiO2, while residual YbAS glass underwent local crystallization, contributing to the formation of a nanoscale multiphase interfacial structure. Overall, A-D-SS retained structural integrity and effectively restricted sustained water-oxygen penetration, demonstrating its potential as an all-oxide bond coat for SiCf/SiC composites.
KW - All-oxide bond coats
KW - SiC/SiC composites
KW - Water-oxygen corrosion
KW - Yb-Al-Si-O glass
UR - https://www.scopus.com/pages/publications/105053738491
U2 - 10.1016/j.corsci.2026.114353
DO - 10.1016/j.corsci.2026.114353
M3 - 文章
AN - SCOPUS:105053738491
SN - 0010-938X
VL - 273
JO - Corrosion Science
JF - Corrosion Science
M1 - 114353