Bending creep test (based on overhang beam geometry) is investigated by incorporating the important contribution of residual stress. Finite element simulations considering the residual stress is employed to investigate the residual stress behavior of bending creep specimen. We propose several methods to determine the creep parameters directly from the bending creep tests. We considered two cases of residual stress, one is tensile residual stress. The other is compressive residual stress. The present work may shed some light on the influences during bending creep, as well as provide an efficient way to determine material residual stress characteristics.

源语言英语
页(从-至)1592-1599
页数8
期刊Measurement: Journal of the International Measurement Confederation
46
4
DOI
出版状态已出版 - 5月 2013

学术指纹

探究 'Investigation of bending creep tests. Part I: Effect of residual stress' 的科研主题。它们共同构成独一无二的学术指纹。

引用此