跳到主要导航 跳到搜索 跳到主要内容

Infrared emissivity change of superalloy K424 with deposited au film

  • Zhibin Huang
  • , Dongmei Zhu
  • , Xiufeng Tang
  • , Wancheng Zhou
  • , Fa Luo
  • Northwestern Polytechnical University Xian

科研成果: 期刊稿件文章同行评审

4 引用 (Scopus)

摘要

The change and its mechanism of the infrared emissivity of superalloy K424 with deposited Au film before and after heat treatment were investigated. XRD analyses show that the metal elements of the substrate diffused from the alloy into the Au film, and mainly formed the solid solution of Cr in Au, i.e. Au0.7Cr0.3. EDXS analyses show that oxides of substrate metal element were formed on the rough surface of the sample with deposited Au film after heat treatment; while the polished surface of the sample was still Au film. Both the surface state and heat treatment have great influence on the infrared emissivity tested by spectral radiometer, SR5000.

源语言英语
页(从-至)1402-1405
页数4
期刊Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering
38
8
出版状态已出版 - 8月 2009

指纹

探究 'Infrared emissivity change of superalloy K424 with deposited au film' 的科研主题。它们共同构成独一无二的指纹。

引用此