TY - JOUR
T1 - Influence of tempering treatment on the microstructure evolution and mechanical properties of laser-cladding high-strength iron-based alloy coatings
AU - Wang, Xinghua
AU - Ding, Rui
AU - Hu, Chenghui
AU - Yang, Dezhen
AU - Wu, Yanming
AU - Liu, Liming
AU - Lin, Xin
N1 - Publisher Copyright:
© 2025 The Authors.
PY - 2025/9/1
Y1 - 2025/9/1
N2 - Achieving crack-resistant, thick laser-clad coatings with balanced strength-crack restraining remains challenging. This study presents a novel Fe-based alloy composition enabling the successful laser cladding of a crack-free, ∼3-mm-thick coating on 38CrMoAl steel. We explicitly investigate the effect of tempering temperature on microstructure evolution and mechanical properties, revealing unique mechanisms critical for thick coatings. Comprehensive characterization (SEM, TEM, XRD, microhardness, wear testing) shows the as-deposited coating consists of martensite, MC/M2C eutectic carbides, and M-A islands, achieving 881.2 HV0.5 hardness. The key novelty lies in the distinct microstructural response to tempering: At 450 °C, M2C decomposition forms fine M6C/MC carbides and austenite reversal significantly increases retained austenite (RA), reducing hardness. At 500 °C, however, MC carbide dissolution (blocky → herringbone) and RA decomposition occur synergistically. This combined transformation drastically reduces RA fraction while refining the carbide morphology, enabling a hardness peak (927 ± 15 HV0.5, +5.2 %) and superior wear resistance (avg. friction coefficient 0.73, +21.7 %). Our findings demonstrate that optimizing tempering temperature to simultaneously trigger RA decomposition and carbide refinement is essential for enhancing thick Fe-based coatings, providing a new pathway for achieving high hardness and wear resistance without cracking.
AB - Achieving crack-resistant, thick laser-clad coatings with balanced strength-crack restraining remains challenging. This study presents a novel Fe-based alloy composition enabling the successful laser cladding of a crack-free, ∼3-mm-thick coating on 38CrMoAl steel. We explicitly investigate the effect of tempering temperature on microstructure evolution and mechanical properties, revealing unique mechanisms critical for thick coatings. Comprehensive characterization (SEM, TEM, XRD, microhardness, wear testing) shows the as-deposited coating consists of martensite, MC/M2C eutectic carbides, and M-A islands, achieving 881.2 HV0.5 hardness. The key novelty lies in the distinct microstructural response to tempering: At 450 °C, M2C decomposition forms fine M6C/MC carbides and austenite reversal significantly increases retained austenite (RA), reducing hardness. At 500 °C, however, MC carbide dissolution (blocky → herringbone) and RA decomposition occur synergistically. This combined transformation drastically reduces RA fraction while refining the carbide morphology, enabling a hardness peak (927 ± 15 HV0.5, +5.2 %) and superior wear resistance (avg. friction coefficient 0.73, +21.7 %). Our findings demonstrate that optimizing tempering temperature to simultaneously trigger RA decomposition and carbide refinement is essential for enhancing thick Fe-based coatings, providing a new pathway for achieving high hardness and wear resistance without cracking.
KW - Fe-based alloy coating
KW - Laser cladding
KW - Mechanical properties
KW - Microstructural evolution
KW - Tempering temperature
UR - https://www.scopus.com/pages/publications/105024420093
U2 - 10.1016/j.jmrt.2025.08.210
DO - 10.1016/j.jmrt.2025.08.210
M3 - 文章
AN - SCOPUS:105024420093
SN - 2238-7854
VL - 38
SP - 4662
EP - 4675
JO - Journal of Materials Research and Technology
JF - Journal of Materials Research and Technology
ER -