N2 - TiAl/Ti2AlNb laminated composites were fabricated by vacuum hot-pack rolling, forming three distinct interfacial regions: brittle regions I (βo + α2 + γ + ω) and II (βo/B2 + α2 + ω), and ductile region III (O). Multiscale characterization combining digital image correlation and in-situ three-point bending tests revealed that the laminated composites exhibit a 2.0–2.5-fold improvement in fracture toughness compared with monolithic TiAl alloy. This enhancement arises from the synergy between intrinsic and extrinsic toughening mechanisms. The intrinsic toughening is associated with slip deformation of B2 grains in the Ti2AlNb layer and grain-boundary obstruction to crack propagation, whereas the extrinsic toughening originates from interfacial crack branching in regions I and II, together with crack deflection and blunting in region III. Furthermore, the critical role of the pre-notch position was emphasized. When the notch terminates in the Ti2AlNb layer, interfacial crack branching effectively alleviates stress concentration, increasing KQ to 40.2 MPa m1/2. Conversely, when the notch terminates in the TiAl layer, rapid crack initiation caused by the low damage tolerance of TiAl triggers premature structural instability, reducing KQ to 29.5 MPa m1/2. These findings provide guidance for interfacial design and toughening optimization of TiAl-based laminated composites.
AB - TiAl/Ti2AlNb laminated composites were fabricated by vacuum hot-pack rolling, forming three distinct interfacial regions: brittle regions I (βo + α2 + γ + ω) and II (βo/B2 + α2 + ω), and ductile region III (O). Multiscale characterization combining digital image correlation and in-situ three-point bending tests revealed that the laminated composites exhibit a 2.0–2.5-fold improvement in fracture toughness compared with monolithic TiAl alloy. This enhancement arises from the synergy between intrinsic and extrinsic toughening mechanisms. The intrinsic toughening is associated with slip deformation of B2 grains in the Ti2AlNb layer and grain-boundary obstruction to crack propagation, whereas the extrinsic toughening originates from interfacial crack branching in regions I and II, together with crack deflection and blunting in region III. Furthermore, the critical role of the pre-notch position was emphasized. When the notch terminates in the Ti2AlNb layer, interfacial crack branching effectively alleviates stress concentration, increasing KQ to 40.2 MPa m1/2. Conversely, when the notch terminates in the TiAl layer, rapid crack initiation caused by the low damage tolerance of TiAl triggers premature structural instability, reducing KQ to 29.5 MPa m1/2. These findings provide guidance for interfacial design and toughening optimization of TiAl-based laminated composites.
KW - Crack propagation
KW - In-situ three-point bending
KW - Interfacial phase transformation
KW - Strengthening and toughening mechanism
KW - TiAl/TiAlNb laminated composites
UR - https://www.scopus.com/pages/publications/105048487576
U2 - 10.1016/j.jmst.2026.08.012
DO - 10.1016/j.jmst.2026.08.012
M3 - 文章
AN - SCOPUS:105048487576
SN - 1005-0302
VL - 285
SP - 303
EP - 313
JO - Journal of Materials Science and Technology
JF - Journal of Materials Science and Technology
ER -