T1 - High temperature tribological behavior of in-situ ceramic-reinforced TiMoNb refractory multi-principal alloy-based composites
AU - Hu, Mingchuan
AU - Zhang, Yufeng
AU - Wang, Hanming
AU - Du, Yin
AU - Liu, Zhifang
AU - Pei, Xuhui
AU - Zhang, Li
AU - Bou-Saïd, Benyebka
AU - Wang, Haifeng
N1 - Publisher Copyright:
© 2026 Elsevier B.V.
PY - 2026/12/15
Y1 - 2026/12/15
N2 - In-situ ceramic reinforcement offers an effective strategy to enhance the tribological performance of refractory multi-principal element alloys (RMPEAs). In this work, TiMoNb(SiC) x ( x molar ratio, x = 0, 0.1, 0.2 and 0.3) composites were fabricated by spark plasma sintering, enabling the in-situ formation of TiC and (Ti, Nb)5Si3 phases. The TiMoNb(SiC)0.2 composite exhibits the lowest and most stable wear rate, reaching 2.69 × 10−6 mm3/Nm even at 800 °C, approximately one order of magnitude lower than the base alloy. Below 300 °C, abrasive wear accompanied by adhesive wear dominates the wear process, the in-situ ceramic reinforcements enhance the deformation resistance of the composites and effectively reduce the severity of adhesive wear. With increasing temperature, oxidative wear gradually becomes predominant. For the TiMoNb(SiC)0.2 composite, a dense self-organized TiO2/SiO2 nano ultrafine-grained tribo-layer forms on the worn surface, which suppresses material removal and may also hinder oxidation diffusion, thereby contributing to its excellent high-temperature tribological stability. These findings provide useful guidance for the design of RMPEA-based composites with superior wear resistance over wide temperature ranges.
AB - In-situ ceramic reinforcement offers an effective strategy to enhance the tribological performance of refractory multi-principal element alloys (RMPEAs). In this work, TiMoNb(SiC) x ( x molar ratio, x = 0, 0.1, 0.2 and 0.3) composites were fabricated by spark plasma sintering, enabling the in-situ formation of TiC and (Ti, Nb)5Si3 phases. The TiMoNb(SiC)0.2 composite exhibits the lowest and most stable wear rate, reaching 2.69 × 10−6 mm3/Nm even at 800 °C, approximately one order of magnitude lower than the base alloy. Below 300 °C, abrasive wear accompanied by adhesive wear dominates the wear process, the in-situ ceramic reinforcements enhance the deformation resistance of the composites and effectively reduce the severity of adhesive wear. With increasing temperature, oxidative wear gradually becomes predominant. For the TiMoNb(SiC)0.2 composite, a dense self-organized TiO2/SiO2 nano ultrafine-grained tribo-layer forms on the worn surface, which suppresses material removal and may also hinder oxidation diffusion, thereby contributing to its excellent high-temperature tribological stability. These findings provide useful guidance for the design of RMPEA-based composites with superior wear resistance over wide temperature ranges.
KW - Composites
KW - In-situ ceramic phases
KW - Multi-principal element alloys
KW - Tribological properties
KW - Wear mechanisms
UR - https://www.scopus.com/pages/publications/105052241695
U2 - 10.1016/j.wear.2026.207064
DO - 10.1016/j.wear.2026.207064
M3 - 文章
AN - SCOPUS:105052241695
SN - 0043-1648
VL - 607
JO - Wear
JF - Wear
M1 - 207064
ER -