N2 - The compression rheological behavior of Mo-12Si-8.5B alloy reinforced by layered Mo2TiAlC2 phase is studied at temperatures ranging from 1200℃ to 1400℃ and strain rates ranging from 0.01s-1 to 0.0001s-1. The trend of flow stress and microstructure evolution was investigated. The results show that the Mo2TiAlC2 strengthens the Mo-12Si-8.5B alloy mainly by particle strengthening and grain boundary strengthening at high temperatures, with the increase of Mo2TiAlC2 content, the peak stress of alloy improved by 43.8% at most. With the increase of test temperature or the decrease of strain rate, the peak stress of alloys decreases significantly. The microstructural observations reveal that the deformation of Mo-12Si-8.5B-Mo2TiAlC2 alloy at high temperatures is mainly provided by the plastic deformation of the soft α-Mo phase and grain boundary sliding. As the temperature rises to 1300℃-1400℃, the intermetallic phase gradually participates in the deforming, however, it contributes less to the total deformation, while dynamic recovery and recrystallization greatly reduce dislocations, and the deformed α-Mo grains are re-equiaxed. The Mo2TiAlC2 particles can inhibit dynamic recrystallization grain growth to some extent.
AB - The compression rheological behavior of Mo-12Si-8.5B alloy reinforced by layered Mo2TiAlC2 phase is studied at temperatures ranging from 1200℃ to 1400℃ and strain rates ranging from 0.01s-1 to 0.0001s-1. The trend of flow stress and microstructure evolution was investigated. The results show that the Mo2TiAlC2 strengthens the Mo-12Si-8.5B alloy mainly by particle strengthening and grain boundary strengthening at high temperatures, with the increase of Mo2TiAlC2 content, the peak stress of alloy improved by 43.8% at most. With the increase of test temperature or the decrease of strain rate, the peak stress of alloys decreases significantly. The microstructural observations reveal that the deformation of Mo-12Si-8.5B-Mo2TiAlC2 alloy at high temperatures is mainly provided by the plastic deformation of the soft α-Mo phase and grain boundary sliding. As the temperature rises to 1300℃-1400℃, the intermetallic phase gradually participates in the deforming, however, it contributes less to the total deformation, while dynamic recovery and recrystallization greatly reduce dislocations, and the deformed α-Mo grains are re-equiaxed. The Mo2TiAlC2 particles can inhibit dynamic recrystallization grain growth to some extent.
KW - Microstructure evolution
KW - Mo-Si-B alloy
KW - MoTiAlC2 phase
KW - Rheological behavior
UR - https://www.scopus.com/pages/publications/105001648013
U2 - 10.2497/jjspm.16P-T14-09
DO - 10.2497/jjspm.16P-T14-09
M3 - 文章
AN - SCOPUS:105001648013
SN - 0532-8799
VL - 72
SP - S1541-S1548
JO - Funtai Oyobi Fummatsu Yakin/Journal of the Japan Society of Powder and Powder Metallurgy
JF - Funtai Oyobi Fummatsu Yakin/Journal of the Japan Society of Powder and Powder Metallurgy
ER -