摘要
The microstructural evolution and mechanical properties of Ti35 alloy applied in nuclear industry with lamellar microstructure during high-temperature straining were systematically investigated. Ti35 alloy plates were subjected to hot rolling down to 20 %, 50 % and 80 % reduction in thickness. Results showed that {101̅2}<101̅1̅>, {112̅2}<112̅3̅>and {101̅1}<101̅2̅>twins were developed during hot rolling and their proportion varied with the amount of deformation. The fraction of twinning boundary reached peak value in the 50 % reduction sample, which dominated by {101̅2}<101̅1̅>and {112̅2}<112̅3̅>twins. After annealing, the deformation twins in>50 % reduction samples were nearly annihilated. The twins and substructures acted as nucleation point for static recrystallization, resulting in twins annihilated and grain refinement during annealing. Micro-hardness and tensile tests revealed that deformation twinning improved strength and plasticity of the Ti35 alloy by introducing extra interfaces and reorientation.
| 源语言 | 英语 |
|---|---|
| 期刊论文编号 | 166670 |
| 期刊 | Journal of Alloys and Compounds |
| 卷 | 925 |
| DOI | |
| 出版状态 | 已出版 - 5 12月 2022 |
| 已对外发布 | 是 |
学术指纹
探究 'Formation and annihilation of deformation twinning in hexagonal Ti with lamellar microstructure' 的科研主题。它们共同构成独一无二的学术指纹。引用此
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver