TY - JOUR
T1 - Exceptional high-temperature performance of Ni-based superalloy by orientation optimizing and grain boundary strengthening via ultrasonic modulation
AU - Hu, Y. J.
AU - Wang, J. Y.
AU - Fan, Z. K.
AU - Zhai, W.
AU - Wei, B.
N1 - Publisher Copyright:
© 2026 Elsevier B.V.
PY - 2026/8/15
Y1 - 2026/8/15
N2 - Modulated ultrasound was applied during thermal preservation and directional solidification of a Ni-based superalloy. Primary γ columnar grains were refined with more concentrated [001] crystallographic texture. Their average grain width was reduced to 58% of that under statically directional solidification, with orientation deviation angle decreasing from 31° to 16°. Low-angle grain boundaries (LAGBs) proportion increased by 2.6 times and their density rose by one order of magnitude. During thermal preservation, transient cavitation induced local high undercooling reaching 81 K to promote nucleation. During subsequent solidification, a refined-γ-grains layer formed without destabilizing solid/liquid interface, introducing higher initial misorientation to accelerate competitive growth. This generated refined and orientated columnar grains, stabilized by a gentle flow field enhancing solute transportation. Near ultrasound-regulated LAGBs, larger boundary density facilitated MC carbides nucleation, making them homogenized with nearly-spherical shape. Lower interface energy inhibited precipitated γ′ coarsening along LAGBs, transforming it from spindle to cubic shape. The creep rupture life after ultrasonic processing reached 196 and 271 h under 1123 K/511 MPa and 1223 K/250 MPa, respectively, extended by the factors of 2.3 and 3.1 compared with static condition. Orientation optimizing lowered the driving force for dislocation glide while strengthened LAGBs promoted dislocation storage ability, shifting the creeping mode from dislocation lines climbing through γ/γ′ channel to network tangling within γ′ phase. The tensile strength and elongation rate at 293 and 1123 K also showed a synergy improvement due to grain boundaries strengthening and stacking faults reinforcement.
AB - Modulated ultrasound was applied during thermal preservation and directional solidification of a Ni-based superalloy. Primary γ columnar grains were refined with more concentrated [001] crystallographic texture. Their average grain width was reduced to 58% of that under statically directional solidification, with orientation deviation angle decreasing from 31° to 16°. Low-angle grain boundaries (LAGBs) proportion increased by 2.6 times and their density rose by one order of magnitude. During thermal preservation, transient cavitation induced local high undercooling reaching 81 K to promote nucleation. During subsequent solidification, a refined-γ-grains layer formed without destabilizing solid/liquid interface, introducing higher initial misorientation to accelerate competitive growth. This generated refined and orientated columnar grains, stabilized by a gentle flow field enhancing solute transportation. Near ultrasound-regulated LAGBs, larger boundary density facilitated MC carbides nucleation, making them homogenized with nearly-spherical shape. Lower interface energy inhibited precipitated γ′ coarsening along LAGBs, transforming it from spindle to cubic shape. The creep rupture life after ultrasonic processing reached 196 and 271 h under 1123 K/511 MPa and 1223 K/250 MPa, respectively, extended by the factors of 2.3 and 3.1 compared with static condition. Orientation optimizing lowered the driving force for dislocation glide while strengthened LAGBs promoted dislocation storage ability, shifting the creeping mode from dislocation lines climbing through γ/γ′ channel to network tangling within γ′ phase. The tensile strength and elongation rate at 293 and 1123 K also showed a synergy improvement due to grain boundaries strengthening and stacking faults reinforcement.
KW - Directional solidification
KW - Mechanical property
KW - Microstructure evolution
KW - Modulated ultrasound
KW - Ni-based superalloy
UR - https://www.scopus.com/pages/publications/105046092697
U2 - 10.1016/j.jallcom.2026.190037
DO - 10.1016/j.jallcom.2026.190037
M3 - 文章
AN - SCOPUS:105046092697
SN - 0925-8388
VL - 1079
JO - Journal of Alloys and Compounds
JF - Journal of Alloys and Compounds
M1 - 190037
ER -