摘要
To investigate the corrosion failure behavior and mechanism of environmental barrier coatings at high temperatures, coatings of Si-Yb2Si2O7-Er2SiO5 system were prepared on continuous silicon carbide fiber-reinforced silicon carbide based ceramic matrix composites by atmospheric plasma spraying, and water oxygen corrosion and molten calcium-magnesium-aluminum-silicate corrosion assessment experiments were conducted at 1 350℃. The failure behavior and the evolution of microstructure and phase composition of the environmental barrier coating during corrosion were studied by XRD, SEM, EDS. The results showed that in water vapor corrosion, Er3Al5O12 and Er(OH)3 generated by the reaction of Er2SiO5 with H2O and Al(OH)3 increased continuously, the volatilization of Er(OH)3 increased the coating porosity, promoting further infiltration of water vapor and internal corrosion. Meanwhile, the generated Er3Al5O12 phase had a thermal expansion mismatch with the coating matrix, generating significant internal stress during thermal cycling. The coupling effect of chemical corrosion and physical stress ultimately led to the formation of longitudinal cracks throughout the entire coating, resulting in coating failure. In CMAS corrosion, Er2SiO5 reacts with CMAS to form apatite and garnet phases, which hinder the infiltration of calcium-magnesium-aluminosilicate (CMAS) melt. However, due to the mismatch between the product and the thermal expansion coefficient of the coating, longitudinal cracks appeared in the coating, but the coating structure remained intact and did not peel off.
| 投稿的翻译标题 | Research on water vapor/calcium-magnesium-aluminum-silicate corrosion failure behavior and mechanisms of Er-based rare earth silicate environmental barrier coating |
|---|---|
| 源语言 | 繁体中文 |
| 页(从-至) | 5233-5242 |
| 页数 | 10 |
| 期刊 | Fuhe Cailiao Xuebao/Acta Materiae Compositae Sinica |
| 卷 | 43 |
| 期 | 8 |
| DOI | |
| 出版状态 | 已出版 - 8月 2026 |
关键词
- CMAS corrosion
- ceramic-matrix composites
- environmental barrier coatings
- rare earth silicates
- water vapor corrosion
学术指纹
探究 'Er 系稀土硅酸盐环境障涂层水氧/钙镁铝硅酸盐腐蚀失效行为及机制' 的科研主题。它们共同构成独一无二的学术指纹。引用此