Energy-Storage Properties of 0.89Bi0.5Na0.5TiO 3-0.06BaTiO3-0.05K0.5Na0.5NbO 3 Lead-Free Anti-ferroelectric Ceramics

  • Feng Gao
  • , Xianlin Dong
  • , Chaoliang Mao
  • , Wei Liu
  • , Hongling Zhang
  • , Lihui Yang
  • , Fei Cao
  • , Genshui Wang
  • CAS - Shanghai Institute of Ceramics

科研成果: 期刊稿件文章同行评审

309 引用 (Scopus)

摘要

Energy-storage properties of 0.89Bi0.5Na0.5TiO 3-0.06BaTiO3-0.05K0.5Na0.5NbO 3 (0.89BNT-0.06BT-0.05KNN) lead-free ceramics were first investigated. Measurements of dielectric properties together with switching current curves indicate a rather diffuse ferroelectric (FE) to anti-ferroelectric (AFE) phase transition when heating from 20°C to 90°C. The energy density (W), which was calculated from P-E hysteresis loops, increases linearly with the external electric field when E exceeds AFE-FE transition field. W is independent of temperature and frequency, and maintains around 0.59 J/cm3 under 5.6 kV/mm in the stable AFE phase region. These properties indicate that 0.89BNT-0.06BT-0.05KNN ceramics might be a promising lead-free AFE material for energy-storage capacitor application.

源语言英语
页(从-至)4382-4386
页数5
期刊Journal of the American Ceramic Society
94
12
DOI
出版状态已出版 - 12月 2011