摘要
The microstructure features of a kind of Ni-Cr-W superalloy after solution heat treatment at different temperatures (1230-1300°C) for various time (10-120 min) were investigated by means of scanning electron microscope (SEM), transmission electron microscopy (TEM) and X-ray diffraction (XRD). The results show that the precipitated phases of the alloy after solution heat treatment are identified as W-rich fcc M6C and Cr-rich fcc M23C6 carbides. The volume fraction of carbides decreases with increasing of the solution heat treatment temperature and time. At the temperature above 1270°C for 120 min, most of carbides are dissolved into the Ni-matrix, and the carbides distributing at twin boundaries may be dissolved into the matrix first. M6C carbide has no any fixed orientation relationship with the Ni-matrix, but the angle of M23C6 (220) to the matrix (13̄1) is 30°.
| 源语言 | 英语 |
|---|---|
| 页(从-至) | 1157-1161 |
| 页数 | 5 |
| 期刊 | Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering |
| 卷 | 39 |
| 期 | 7 |
| 出版状态 | 已出版 - 7月 2010 |
指纹
探究 'Effects of solution heat treatment on carbide of Ni-Cr-W superalloy' 的科研主题。它们共同构成独一无二的指纹。引用此
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver