TY - JOUR
T1 - Effect of two-step stabilization routes on the microstructure and tensile properties of a W-modified Ti-643s alloy at room temperature and 600°C
T2 - Multiphase strengthening and deformation compatibility
AU - Xia, Wenhao
AU - Li, Fuguo
AU - Wan, Miaomiao
AU - Yao, Kenan
AU - Huang, Weiming
AU - Xu, Jianwei
N1 - Publisher Copyright:
© 2026 Elsevier B.V.
PY - 2026/10/31
Y1 - 2026/10/31
N2 - An investigation was carried out on an unreported W-modified Ti-643s alloy to elucidate the impact of representative thermal stabilization routes on the alloy's microstructural evolution and mechanical performance, with the aim of identifying a suitable processing window for elevated-temperature applications. A comparative analysis of three prototypical thermal stabilization (TS) treatments was performed. Among the investigated conditions, TS-II exhibited the most favorable overall mechanical performance. The room-temperature strength–ductility product increased by 66.7% relative to the forged condition, while the tensile strength at 600°C reached 650 ± 10 MPa with an elongation of 35.5 ± 1.2%. The superior performance of TS-II is associated with its more favorable multiphase architecture. This architecture is characterized by a distribution and coordination of primary αp, secondary αs, and transformed β phases that are more favorable for strengthening and strain accommodation. Taylor factor analysis further suggests that the enhanced performance is closely associated with the improved deformation compatibility, which is attributable to a more suitable distribution of grain orientations. These results identify TS-II as the preferred thermal stabilization route for the present alloy and demonstrate the potential of this newly designed Ti-643s alloy for short-term elevated-temperature applications.
AB - An investigation was carried out on an unreported W-modified Ti-643s alloy to elucidate the impact of representative thermal stabilization routes on the alloy's microstructural evolution and mechanical performance, with the aim of identifying a suitable processing window for elevated-temperature applications. A comparative analysis of three prototypical thermal stabilization (TS) treatments was performed. Among the investigated conditions, TS-II exhibited the most favorable overall mechanical performance. The room-temperature strength–ductility product increased by 66.7% relative to the forged condition, while the tensile strength at 600°C reached 650 ± 10 MPa with an elongation of 35.5 ± 1.2%. The superior performance of TS-II is associated with its more favorable multiphase architecture. This architecture is characterized by a distribution and coordination of primary αp, secondary αs, and transformed β phases that are more favorable for strengthening and strain accommodation. Taylor factor analysis further suggests that the enhanced performance is closely associated with the improved deformation compatibility, which is attributable to a more suitable distribution of grain orientations. These results identify TS-II as the preferred thermal stabilization route for the present alloy and demonstrate the potential of this newly designed Ti-643s alloy for short-term elevated-temperature applications.
KW - 600°C tensile properties
KW - Multiphase strengthening
KW - Strength–ductility synergy
KW - Thermal stabilization
KW - Tungsten-modified titanium alloy
UR - https://www.scopus.com/pages/publications/105051753338
U2 - 10.1016/j.jallcom.2026.191393
DO - 10.1016/j.jallcom.2026.191393
M3 - 文章
AN - SCOPUS:105051753338
SN - 0925-8388
VL - 1082
JO - Journal of Alloys and Compounds
JF - Journal of Alloys and Compounds
M1 - 191393
ER -