跳到主要导航 跳到搜索 跳到主要内容

Effect of SiC nanowires on the thermal shock resistance of joint between carbon/carbon composites and Li2O-Al2O3-SiO2 glass ceramics

  • Northwestern Polytechnical University Xian

科研成果: 期刊稿件 › 文章 › 同行评审

27 引用 (Scopus)

摘要

In order to improve the bonding property of joint between SiC modified carbon/carbon (C/C) composites and Li2O-Al2O3-SiO2 (LAS) glass ceramics, SiC nanowires were attempted as the reinforcement materials in the interface region of SiC transition layer and Li2O-MgO-Al2O3-SiO2 (LMAS) gradient joining interlayer. The C/C-LAS joint with SiC nanowire-reinforced interface layer was prepared by a three-step technique of pack cementation, in situ reaction and hot-pressing. The microstructure and thermal shock resistance of the as-prepared joints were examined. The average shear strength of the joined samples with SiC nanowires increased from 24.9MPa to 31.6MPa after 40 thermal cycles between 1000°C and room temperature, while that of the joined samples without SiC nanowires dropped from 21.4MPa to 8.3MPa. The increase of thermal shock resistance of the C/C-LAS joints was mainly attributed to the toughening mechanism of SiC nanowires by pullout, bridging and crack deflection.

源语言英语
页(从-至)2535-2541
页数7
期刊Journal of the European Ceramic Society
卷34
期10
DOI
出版状态已出版 - 9月 2014

学术指纹

探究 'Effect of SiC nanowires on the thermal shock resistance of joint between carbon/carbon composites and Li2O-Al2O3-SiO2 glass ceramics' 的科研主题。它们共同构成独一无二的学术指纹。

引用此