TY - JOUR
T1 - Effect of heat treatment on microstructure and fracture toughness of Nb-15Si-22 (Ti + Zr) refractory alloy via laser-directed energy deposition
AU - Li, Yunlong
AU - Zhang, Zirun
AU - Xie, Yong
AU - Yun, Jun
AU - Lin, Xin
AU - Zhao, Zhanyong
AU - Du, Wenbo
AU - Bai, Peikang
N1 - Publisher Copyright:
© 2026 Elsevier Ltd. All rights are reserved, including those for text and data mining, AI training, and similar technologies.
PY - 2026/12
Y1 - 2026/12
N2 - Laser-directed energy deposition (L-DED) was employed to fabricate Nb-15Si-22 (Ti + Zr) refractory alloys with four different combinations of Ti and Zr additions. The influence of heat treatment (1400 °C for 30 h) on their microstructure and room-temperature mechanical properties was systematically investigated. In the as-deposited state, substituting Ti with Zr promotes the transformation from metastable Nb3Si to stable γ-Nb5Si3, refines the eutectic structure, and forms a continuous Nbss+γ-Nb5Si3 network. After heat treatment, Nb3Si fully decomposes, the volume fraction of γ-Nb5Si3 increases markedly, and the dominant orientation relationship between Nbss and γ-Nb5Si3 evolves to {110} Nbss//{0001} γ, which lowers interfacial energy and enhances phase bonding. Microhardness decreases monotonically with increasing Zr content and drops further after heat treatment. Fracture toughness first increases and then decreases with Zr addition; the 14Ti8Zr alloy achieves the highest KQ of 15.1 MPa·m1/2 after heat treatment. Moderate Zr addition effectively activates multiple extrinsic toughening mechanisms- crack deflection, branching, and bridging- leading to a transition from brittle transgranular cleavage to ductile interphase tearing. This work elucidates the synergistic effects of relative amounts of Ti and Zr, and heat treatment on microstructure-property correlations in L-DED processed Nb-Si-based refractory alloys.
AB - Laser-directed energy deposition (L-DED) was employed to fabricate Nb-15Si-22 (Ti + Zr) refractory alloys with four different combinations of Ti and Zr additions. The influence of heat treatment (1400 °C for 30 h) on their microstructure and room-temperature mechanical properties was systematically investigated. In the as-deposited state, substituting Ti with Zr promotes the transformation from metastable Nb3Si to stable γ-Nb5Si3, refines the eutectic structure, and forms a continuous Nbss+γ-Nb5Si3 network. After heat treatment, Nb3Si fully decomposes, the volume fraction of γ-Nb5Si3 increases markedly, and the dominant orientation relationship between Nbss and γ-Nb5Si3 evolves to {110} Nbss//{0001} γ, which lowers interfacial energy and enhances phase bonding. Microhardness decreases monotonically with increasing Zr content and drops further after heat treatment. Fracture toughness first increases and then decreases with Zr addition; the 14Ti8Zr alloy achieves the highest KQ of 15.1 MPa·m1/2 after heat treatment. Moderate Zr addition effectively activates multiple extrinsic toughening mechanisms- crack deflection, branching, and bridging- leading to a transition from brittle transgranular cleavage to ductile interphase tearing. This work elucidates the synergistic effects of relative amounts of Ti and Zr, and heat treatment on microstructure-property correlations in L-DED processed Nb-Si-based refractory alloys.
KW - Fracture toughness
KW - Heat treatment
KW - Laser-directed energy deposition
KW - Microstructure
KW - NbSi based alloy
UR - https://www.scopus.com/pages/publications/105048707392
U2 - 10.1016/j.ijrmhm.2026.108074
DO - 10.1016/j.ijrmhm.2026.108074
M3 - 文章
AN - SCOPUS:105048707392
SN - 0263-4368
VL - 141
JO - International Journal of Refractory Metals and Hard Materials
JF - International Journal of Refractory Metals and Hard Materials
M1 - 108074
ER -